Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 1.36 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.30 - 1.36 g/cc
1.30 - 1.36 g/cc
ASTM D792
S&E Specialty Polymers TufTech™ GA-1050-02LF PVC Compound
Application: A 105°C, AWM, 90°C AWM 1,000 volt, flame retardant compound.Information provided by S&E Specialty Polymers
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
NBR NM-IEC 60811-1-3
Karina E MCP 520 Black PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
NBR NM-IEC 60811-1-3
Karina E810-40/312-IS-RG Green PVC Compound
Non toxic PVC compound, recommended for blow molding of bottles for alcoholic beverages.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.30 - 1.36 g/cc
1.30 - 1.36 g/cc
NBR NM-IEC 60811-1-3
Karina 36/234-FC-LMP (SDB) Brown Color Concentrate for PVC
Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. ..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D 792
Karina 651D28/29-D-IS ICE PVC Compound
Fungi resistant PVC compound, recommended for injection of bathroom carpet.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.30 - 1.36 g/cc
1.30 - 1.36 g/cc
ASTM D 792
Karina E 18/35-FC-LMP Gray Color Concentrate for PVC
Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. ..
Specific Gravity 1.30 - 1.36 g/cc
1.30 - 1.36 g/cc
ASTM D 792
Karina E 552-48/1-DT-IE Black PVC Compound
Black PVC compound with fruit scent, recommended for shoe sole injection.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.30 - 1.36 g/cc
1.30 - 1.36 g/cc
ASTM D 792
Karina E 74/240-D-IS-SD-TR Compound PVC Crystal
Films laminated shrinkInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.30 - 1.36 g/cc
1.30 - 1.36 g/cc
ASTM D 792
Karina E 74/240-D-IS-SD-TR Compound PVC Crystal
Films, laminated shrinkInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.30 - 1.36 g/cc
1.30 - 1.36 g/cc
NBR NM-IEC 60811-1-3
Karina 750-DM-48/1-B-IS Black PVC Compound
PVC compound recommended for opaque jacketing of retractable telephone wiresInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D792
Compuestos Dominicanos Polycom VN-050485 PVC
Description: Compuestos Dominicanos manufactures the polycom VN products for the extrusion printable sheets and banners having good printing quality.Application: Sheet and bannersAppearance: Natural..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 8571 Moldings & Extrusions Flexible PVC
High quality, semi-rigid extrusion compound especially formulated for extruded T-moldings and other shapes where uniform flow through the die is required.Information provided by Georgia GulfGeorgia ..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 12770 Coax & Telecom Flexible PVC
Non-lead stabilized, CATV and general purpose jacket with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 15643 Wire & Cable Flexible PVC
Non-lead stabilized semi-rigid insulation compound recommended for Style #1061 applications. Maximum service temperature of 105°C. The compound is also formulated for fungus and microbe resistanc..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 16860 Wire & Cable Flexible PVC
Battery booster jacket compound and general purpose jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 18730 Wire & Cable Flexible PVC
UL recognized 720 hour sunlight resistant in all colors, oil resistant, 105 C rated PVC jacket compound with good low temperature performance. Information provided by Georgia GulfGeorgia Gulf became..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 19450 Wire & Cable Flexible PVC
105°C rated insulation compound with very good migration and oil resistance. Recommended for toner resistant applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 2010 Wire & Cable Flexible PVC
General purpose insulation and jacketing compound recommended for 75°C applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 38552 Wire & Cable Flexible PVC
General purpose insulating and jacketing compound for 105°C AWM and SPT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 38702 Moldings & Extrusions Flexible PVC
Flame retardant CATV and general purpose jacket with excellent low temperature properties. UL approved for 720 hour sunlight resistance in all colors. UL approved for 94 V-0 at 1.5 mm in all color..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 4510 Flexible PVC
Non-lead stabilized 105C rated automotive harness compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 11441 Wire & Cable Flexible PVC
Clear extrusion compound formulated for applications necessitating a high degree of flame retardancy.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 19470 Wire & Cable Flexible PVC
Semi-rigid, 105°C insulation compound recommended for a minimum wall thickness of 10 mils. Designed to meet the performance criteria of military spec. MIL-W-16878D.Information provided by Georgia ..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 19473 Wire & Cable Flexible PVC
Non-lead stabilized, 105°C insulation compound recommended for a minimum wall thickness of 10 mils. Designed to meet the performance criteria of military spec. MIL-W-16878D.Information provided by..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 19482 Wire & Cable Flexible PVC
105°C, VW-1 rated non-lead stabilized insulation compound. Ideally suited for 18 AWG, 1/64 wall. UL approved for TW, THW, THHW applications.Information provided by Georgia GulfGeorgia Gulf became..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 19471 Wire & Cable Flexible PVC
Semi-rigid, 105°C insulation compound recommended for a minimum wall thickness of 10 mils. Designed to meet the performance criteria of military spec. MIL-W-16878D.Information provided by Georgia ..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 4441 Flexible PVC
85C non-lead stabilized wire harness. SAE J1128.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 18840 Wire & Cable Flexible PVC
Non-lead stabilized 105C jacket compound for use in SPTO, SJTO and SVTO applications. Best suited for 30 mil walls and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporat..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 38702 Coax & Telecom Flexible PVC
Flame retarded CATV and general purpose jacket with excellent low temperature properties. UL approved for 720 hour sunlight resistance in all colors. UL approved for 94 V-0 at 1.5 mm in all colors..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 8918 Moldings & Extrusions Flexible PVC
Non-lead migration resistant extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Copyright © lookpolymers.com All Rights Reserved