Dow BETADAMP™ 32HT  (discontinued **)

Category Polymer , Thermoset , Epoxy
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow BETADAMP™ 32HT  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
BETADAMP™ 32HT is a high temperature vibration damper that can be applied to the exterior of cast aluminum or steel engine valve, transmission, and crankcase (oil pan) covers or electro-coat substrates in paint shop on interior or exterior applications. BETADAMP™ 32HT has excellent thermal resistance. BETADAMP™ 32HT is epoxy base material containing no Poly Vinyl Chloride (PVC). Information provided by Dow
Physical Properties Metric English Comments
Specific Gravity 1.30 - 1.36 g/cc
1.30 - 1.36 g/cc
Solids Content >= 99.5 %
>= 99.5 %
3 hr @ 105°C
Viscosity Measurement 145 - 189
145 - 189
[sec], 0.052" orifice, 40psi, 20gm
Mechanical Properties Metric English Comments
Adhesive Bond Strength 5.52 MPa
800 psi
Cast aluminum substrate 20 min @ 150°C (MT); ASTM D1002
Descriptive Properties Value Comments
Damping Performance: Composite Loss Factor 0.1
SAE J 1637, 2.5 mm thick, 50°C
0.1
SAE J 1637, 2.5 mm thick, 35°C
0.175
SAE J 1637, 2.5 mm thick, 75°C