Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall 8552 Moldings & Extrusions Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 8552 Moldings & Extrusions Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A soft extrusion compound recommended for profiles, weatherstrips and sheeting. Also suitable for injection molding.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 52 - 58
52 - 58
delayed; ASTM D-2240
Tensile Strength, Yield 8.62 MPa
1250 psi
ASTM D-638
Elongation at Yield 400 %
400 %
ASTM D-638
100% Modulus 0.00293 GPa
0.425 ksi
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 168 °C
335 °F
Users viewing this material also viewed the following: