Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D792 |
S&E Specialty Polymers GA-1941-AFRO PVC Application: 105° C PVC insulating compound designed for SJEOO applicationsInformation provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D792 |
S&E Specialty Polymers GA-509ORLT PVC Application: Lead free, flame retardant UV and oil resistant PVC jacketing compound with superior low temperature properties.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D792 |
S&E Specialty Polymers TufFlex™ GF 3161 PNU TPE Compound Application: High performance oil, gasoline & chemical resistant boot upper compound.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D792 |
S&E Specialty Polymers TufFlex™ GTPE-2272 TPE Compound Application: A 105°C flexible, oil resistant, flame retardant TPE jacketing material designed for SJEO applications.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.10 - 1.30 g/cc | 1.10 - 1.30 g/cc | |
PolyChem Alloy PolyGard 3005R PolyFoam decomposes when heated to create a uniform microcellular structure. It can be used in extrusion and injection molding processes to reduce weight in parts without adversely affecting the ph.. |
|||
Specific Gravity | 0.900 - 1.30 g/cc | 0.900 - 1.30 g/cc | |
Parker Chomerics CHO-SHIELD® 2056 Conductive Coating CHO-SHIELD® 2054 silver-plated-copper filled commercial-grade coating proved high levels of EMI shielding effectiveness, abrasion resistance and excellent adhesion on a variety of materials used fo.. |
|||
Specific Gravity | 1.20 - 1.30 g/cc | 1.20 - 1.30 g/cc | |
PolyChem Alloy AquaGard™ 3004M AquaGard products are designed to improve the flame retardency of polyolefins without the use of halogen additives, such as bromine or chlorine. AquaGard products are available in a polyethylene .. |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D 792 |
Karina 701D25-1-A-IS Natural PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D 792 |
Karina 771-48/1-BY-IS Black PVC Compound Weather resistant PVC compound, recommended for injection and extrusion of automotive profilesInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.26 - 1.30 g/cc | 1.26 - 1.30 g/cc | ASTM D 792 |
Karina 800D48/1-A-IS-BZ Black PVC Compound Heavy metal free PVC compound recommended for injection and extrusion of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D 792 |
Karina 920D32/91 Orange PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D 792 |
Karina E 42/261-GEN Dark Red MBATCH (SP31543) for PVC Recommended usage from 2% to 3% on crystal PVC compoundInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D 792 |
Karina E 57/200-D-AT-IS-SD Clear PVC Compound PVC compound recommended for shrink films.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D 792 |
Karina E 650D35/1-A Ivory PVC Compound For footware/soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D 792 |
Karina E 680D18/487-B-IS Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D 792 |
Karina E 680D35/1-B-IS Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D 792 |
Karina 57/200-D-AT-IS-SD Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.27 - 1.30 g/cc | 1.27 - 1.30 g/cc | ASTM D792 |
Spartech Royalite R522 PVC Alloy Aircraft Grade Sheet Description: Aircraft Grade SheetInformation provided by Spartech. |
|||
Specific Gravity | 1.26 - 1.30 g/cc | 1.26 - 1.30 g/cc | ASTM D792 |
Compuestos Dominicanos Polycom C-051065 PVC Compound Compuestos Dominicanos SA produces a wide variety of PVC compounds for the injection molding of footwear products; everything from full injection, shoe soles, boots, and PVC compounds for oil resist.. |
|||
Specific Gravity | 1.26 - 1.30 g/cc | 1.26 - 1.30 g/cc | ASTM D-792 |
Axiall 8560 Moldings & Extrusions Flexible PVC A clear, semi-rigid extrusion or molding grade compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.26 - 1.30 g/cc | 1.26 - 1.30 g/cc | ASTM D-792 |
Axiall EX1188B Wire & Cable Flexible PVC UL 360 jacket compound. 105°C air; 60°C oil.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.26 - 1.30 g/cc | 1.26 - 1.30 g/cc | ASTM D-792 |
Axiall 11470 Wire & Cable Flexible PVC Highly flame retardant clear compound. Recommended as jacket in PVC/PVC VW-1 constructions.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.26 - 1.30 g/cc | 1.26 - 1.30 g/cc | ASTM D-792 |
Axiall 8710 Moldings & Extrusions Flexible PVC Low gravity extrusion compound with excellent low temperature properties. Designed for use in weatherstrips and flexible gaskets. Excellent for co-extrusion with rigid PVC.Information provided by .. |
|||
Specific Gravity | 1.26 - 1.30 g/cc | 1.26 - 1.30 g/cc | ASTM D-792 |
Axiall 8780 Moldings & Extrusions Flexible PVC Low gravity, general purpose extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.26 - 1.30 g/cc | 1.26 - 1.30 g/cc | ASTM D-792 |
Axiall 19740 Wire & Cable Flexible PVC Non-lead stabilized, 105°C rated insulation compound with excellent low temperature properties. Suitable for use in Class 43 applications. Also suitable for injection molding applications.Informa.. |
|||
Specific Gravity | 0.900 - 1.30 g/cc | 0.900 - 1.30 g/cc | |
Parker Chomerics CHO-SHIELD® 2052 Conductive Coating CHO-SHIELD® 2052 silver-plated-copper filled commercial-grade coating proved high levels of EMI shielding effectiveness, abrasion resistance and excellent adhesion on a variety of materials used fo.. |
|||
Specific Gravity | 1.26 - 1.30 g/cc | 1.26 - 1.30 g/cc | ASTM D-792 |
Axiall 8681 Moldings & Extrusions Flexible PVC General purpose, elastomeric vinyl compound well suited for co-extrusion with rigid PVC.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.26 - 1.30 g/cc | 1.26 - 1.30 g/cc | NBR NM-IEC 60811-1-3 |
Karina 02/223-G Yellow Color Concentrate for PVC Color concentrate recommended for application in PVC compounds for general purposes injection. Recommended to use 2%.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.26 - 1.30 g/cc | 1.26 - 1.30 g/cc | ASTM D 792 |
Karina CAK 55-48/1 Black PVC Compound Reclaimed PVC compound recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.26 - 1.30 g/cc | 1.26 - 1.30 g/cc | ASTM D-792 |
Axiall 18650 Moldings & Extrusions Flexible PVC General purpose compound recommended for 105C applications. Well suited for 105C molding and general purpose extrusions.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in.. |