Material Notes:
Application: A 105°C flexible, oil resistant, flame retardant TPE jacketing material designed for SJEO applications.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.24 - 1.30 g/cc
1.24 - 1.30 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 69.0 - 75.0
<br>@Time 15.0 sec
69.0 - 75.0
<br>@Time 0.00417 hour
ASTM D2240
Tensile Strength 12.4 MPa
1800 psi
ASTM D412
13.268 MPa
<br>@Temperature 100 °C,<br> Time 346000 sec
1924.4 psi
<br>@Temperature 212 °F,<br> Time 96.0 hour
Oil Aged
14.384 MPa
<br>@Temperature 75.0 °C,<br> Time 5.18e+6 sec
2086.2 psi
<br>@Temperature 167 °F,<br> Time 1440 hour
Oil Aged
14.756 MPa
<br>@Temperature 136 °C,<br> Time 605000 sec
2140.2 psi
<br>@Temperature 277 °F,<br> Time 168 hour
Aged
Elongation at Break 300 %
300 %
ASTM D412
195 %
<br>@Treatment Temp. 100 °C,<br> Time 346000 sec
195 %
<br>@Treatment Temp. 212 °F,<br> Time 96.0 hour
Oil Aged
243 %
<br>@Treatment Temp. 75.0 °C,<br> Time 5.18e+6 sec
243 %
<br>@Treatment Temp. 167 °F,<br> Time 1440 hour
Oil Aged
255 %
<br>@Treatment Temp. 136 °C,<br> Time 605000 sec
255 %
<br>@Treatment Temp. 277 °F,<br> Time 168 hour
Aged
Thermal Properties Metric English Comments
Brittleness Temperature -35.0 °C
-31.0 °F
ASTM D746
Oxygen Index 28.0 %
28.0 %
ASTM D2863
Copyright © lookpolymers.com All Rights Reserved