Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall 19740 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 19740 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Non-lead stabilized, 105°C rated insulation compound with excellent low temperature properties. Suitable for use in Class 43 applications. Also suitable for injection molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.26 - 1.30 g/cc
1.26 - 1.30 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 71 - 77
71 - 77
delayed; ASTM D-2240
Tensile Strength, Yield 14.8 MPa
2150 psi
ASTM D-638
Elongation at Yield 309.8 %
309.8 %
Air Aging: 168 hours @ 136°C; 30 mil slabs; UL 1581
350 %
350 %
ASTM D-638
100% Modulus 0.00689 GPa
1.00 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -40.0 °C
-40.0 °F
ASTM D-746
Oxygen Index 24.5 %
24.5 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 177 °C
350 °F
Users viewing this material also viewed the following: