Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.16 - 1.20 g/cc | 1.16 - 1.20 g/cc | ASTM D792 |
S&E Specialty Polymers GM-3255 PVC Application: Non-toxic PVC material designed for molding applications.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.14 - 1.20 g/cc | 1.14 - 1.20 g/cc | ASTM D792 |
S&E Specialty Polymers GTPE-2203G1 PVC Application: RoHS compliant, 105° C, flexible, oil resistant TPE jacketing material with extremely good low temperature properties.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.15 - 1.20 g/cc | 1.15 - 1.20 g/cc | |
Nanocyl EPOCYL™ NC E128-02 Master Batch Liquid Bisphenol-A Resin for non-Solvent Based Formulation Purposes EPOCYL™ NC E128-02 is a Mater Batch based on liquid Bisphenol-A (Bis-A) epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl. It is specifically developed to enh.. |
|||
Specific Gravity | 1.15 - 1.20 g/cc | 1.15 - 1.20 g/cc | |
Nanocyl EPOCYL™ NC E128-04 Master Batch Liquid Bisphenol-A Resin for Solvent Based Formulation Purposes EPOCYL™ NC E128-04 is a Mater Batch based on liquid Bisphenol-A (Bis-A) epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl. It is specifically developed for so.. |
|||
Specific Gravity | 1.15 - 1.20 g/cc | 1.15 - 1.20 g/cc | |
Nanocyl EPOCYL™ NC R128-02 Master Batch Liquid Bisphenol-A Resin for Hot-Melt Formulation Purposes: Dilution Factor 6 EPOCYL™ NC R128-02 is a Master Batch based on liquid Bisphenol-A (Bis-A) epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl, with a suggested dilution factor of.. |
|||
Specific Gravity | 1.15 - 1.20 g/cc | 1.15 - 1.20 g/cc | |
Nanocyl EPOCYL™ NC R128-04 Master Batch Liquid Bisphenol-A Resin for Solvent Based Formulation Purposes: Dilution Factor 6 EPOCYL™ NC R128-04 is a Master Batch based on liquid Bisphenol-A (Bis-A) epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl, with a suggested dilution factor of.. |
|||
Specific Gravity | 1.15 - 1.20 g/cc | 1.15 - 1.20 g/cc | |
Nanocyl EPOCYL™ NC R2HM-01 Formulated Epoxy-Carbon Nanotube Pre-preg Resin System EPOCYL™ NC R2HM-01 is a formulated epoxy based resin system for hot melt pre-preg and pressure molding processes, modified with our own Carbon Nanotubes (CNT), specifically developed to enhance the.. |
|||
Specific Gravity | 1.00 - 1.20 g/cc | 1.00 - 1.20 g/cc | |
PolyChem Alloy FlexGel 4092, 4092D TPE A Zero Shore Hardness TPE, FlexGel is soft, flexible, and resilient, with excellent chemical and moisture resistance. The material can be decorated, printed, reground, and reprocessed without any si.. |
|||
Specific Gravity | 1.00 - 1.20 g/cc | 1.00 - 1.20 g/cc | |
PolyChem Alloy FlexGel 5007HF TPE A Zero Shore Hardness TPE, FlexGel is soft, flexible, and resilient, with excellent chemical and moisture resistance. The material can be decorated, printed, reground, and reprocessed without any si.. |
|||
Specific Gravity | 1.00 - 1.20 g/cc | 1.00 - 1.20 g/cc | |
PolyChem Alloy FlexGel 8307 TPE A Zero Shore Hardness TPE, FlexGel is soft, flexible, and resilient, with excellent chemical and moisture resistance. The material can be decorated, printed, reground, and reprocessed without any si.. |
|||
Specific Gravity | 1.14 - 1.20 g/cc | 1.14 - 1.20 g/cc | ASTM D 792 |
Karina E TR 500D22/173 Honey PVC Compound Honey PVC compound additivated with nitrile rubber, recommended for injection of general soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.02 - 1.20 g/cc | 1.02 - 1.20 g/cc | |
LG Chemical IM810 Acrylic impact modifier Description: LG AIM (Acrylic impact modifier) is a type of additives that improves weather-resistance, impact strength, and processability of thermoplastic resin including PVC, which is used for pro.. |
|||
Specific Gravity | 1.16 - 1.20 g/cc | 1.16 - 1.20 g/cc | ASTM D792 |
LG Chemical LUPOY GP5100 PC/ABS+GF10% Description: Injection Molding, PC/ABS+GF10%, General Purpose, GF ReinforcedApplication: Electrical Appliance Housing, Automotive I/PCAS: 103598-77-2, 9003-56-9 and 65997-17-3Information provided by.. |
|||
Specific Gravity | 1.10 - 1.20 g/cc | 1.10 - 1.20 g/cc | ASTM D792 |
Loxim 840 02T HB Polypropylene Compound, 40% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Specific Gravity | 1.10 - 1.20 g/cc | 1.10 - 1.20 g/cc | ASTM D792 |
Loxim 841 02T HB Polypropylene Compound, 40% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Specific Gravity | 1.14 - 1.20 g/cc | 1.14 - 1.20 g/cc | ASTM D 792 |
Karina 350-02/249 Yellow PVC Compound For footware.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.14 - 1.20 g/cc | 1.14 - 1.20 g/cc | ASTM D 792 |
Karina 550D32/13-AT-IS Orange PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.14 - 1.20 g/cc | 1.14 - 1.20 g/cc | ASTM D 792 |
Karina 550D42/10-AT-IS Red PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.16 - 1.20 g/cc | 1.16 - 1.20 g/cc | ASTM D 792 |
Karina BT-0002/17 White PVC Compound PVC compound with addition of nitrile rubber, recommended for injection of boots, soles, and butcher shop bootsInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.10 - 1.20 g/cc | 1.10 - 1.20 g/cc | IEC 1212-2 7.2 |
Hippe PF CP 21 Cellulose Paper Reinforced Phenolic Resin - Round, Rolled Tube Used in mechanical and low-voltage electrical applications. Good electrical properties when exposed to normal relative humidity.Information provided by Hippe. |
|||
Specific Gravity | 1.10 - 1.20 g/cc | 1.10 - 1.20 g/cc | IEC 1212-2 7.2 |
Hippe PF CP 23 Cellulose Paper Reinforced Phenolic Resin - Round, Rolled Tube Used in mechanical and low-voltage electrical applications. Good electrical properties when exposed to normal and high relative humidity.Information provided by Hippe. |
|||
Specific Gravity | 1.10 - 1.20 g/cc | 1.10 - 1.20 g/cc | IEC 1212-2 7.2 |
Hippe PF CP 24 Cellulose Paper Reinforced Phenolic Resin - Round, Rolled Tube Used in electrical and mechanical applications. Very good electrical properties when exposed to high relative humidity. Much higher mechanical strength and insulation resistance than type PF CP 21.. |
|||
Specific Gravity | 1.16 - 1.20 g/cc | 1.16 - 1.20 g/cc | ASTM D792 |
Compuestos Dominicanos Polycom CH-550055-01 PVC Compound Compuestos Dominicanos SA produces a wide variety of PVC compounds for the injection molding of footwear products; everything from full injection, shoe soles, boots, and PVC compounds for oil resist.. |
|||
Specific Gravity | 1.16 - 1.20 g/cc | 1.16 - 1.20 g/cc | ASTM D792 |
Compuestos Dominicanos Polycom ME-333660 PVC Compound Applications: Seals for caps Appearance: Clear pelletsInformation provided by Compuestos Dominicanos |
|||
Specific Gravity | 1.16 - 1.20 g/cc | 1.16 - 1.20 g/cc | ASTM D-792 |
Axiall 59996J Moldings & Extrusions Flexible PVC Injection and molding compound with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.16 - 1.20 g/cc | 1.16 - 1.20 g/cc | ASTM D-792 |
Axiall 8610 Moldings & Extrusions Flexible PVC A high quality, low gravity, clear extrusion and molding compound with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.14 - 1.20 g/cc | 1.14 - 1.20 g/cc | ASTM D792 |
Buckeye Polymers BP FLEX D6509 CU BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Specific Gravity | 1.16 - 1.20 g/cc | 1.16 - 1.20 g/cc | ASTM D792 |
Buckeye Polymers BP FLEX A6810 BLK Thermoplastic Elastomer SEBS Product Information: BP Flex Thermoplastic Elastomers are based on SEBS polymers (Styrene-ethylene/butylene-styrene) providing increased oxidation and weather resistance, higher service temperatures.. |
|||
Specific Gravity | 1.02 - 1.20 g/cc | 1.02 - 1.20 g/cc | |
LG Chemical IM812 Acrylic impact modifier Description: LG AIM (Acrylic impact modifier) is a type of additives that improves weather-resistance, impact strength, and processability of thermoplastic resin including PVC, which is used for pro.. |
|||
Specific Gravity | 1.16 - 1.20 g/cc | 1.16 - 1.20 g/cc | ASTM D792 |
Compuestos Dominicanos Polycom CO-160355 PVC Compound Compuestos Dominicanos SA produces a wide variety of PVC compounds for the injection molding of footwear products; everything from full injection, shoe soles, boots, and PVC compounds for oil resist.. |