| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | ASTM D792 |
|
Polymax® Maxelast® P2950 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
|
|||
| Specific Gravity | >= 1.00 g/cc | >= 1.00 g/cc | |
|
Parker Chomerics CHO-BOND 1067, Part A Silicone Resin Mixture
Information provided by Chomerics
|
|||
| Specific Gravity | >= 1.00 g/cc | >= 1.00 g/cc | |
|
Parker Chomerics CHO-SEAL 1277 Conductive Elastomer
Information provided by Chomerics
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | ASTM D792 |
|
Quadrant EPP TIVAR® 88 W/BurnGuard, Flame Retardant Lining Material (ASTM Product Data Sheet)
Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl..
|
|||
| Specific Gravity | <= 1.00 g/cc | <= 1.00 g/cc | |
|
Parker Chomerics CHO-SHIELD® 610 Part C Solvent Blend
Information provided by Chomerics
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | Uncured |
|
Permabond F202 Anaerobic Retainer
The unique 'toughening' process incorporated into Permabond® F202 gives this anaerobic adhesive excellent resistance to peel and impact forces. Primarily designed for use on metal surfaces, it is a..
|
|||
| Specific Gravity | >= 1.00 g/cc | >= 1.00 g/cc | |
|
Parker Chomerics CHO-BOND 1011, Part A
Information provided by Chomerics
|
|||
| Specific Gravity | >= 1.00 g/cc | >= 1.00 g/cc | |
|
Parker Chomerics CHO-BOND 4041 Part A Conductive Adhesive
Information provided by Chomerics
|
|||
| Specific Gravity | 1.00 - 1.02 g/cc | 1.00 - 1.02 g/cc | |
|
Michelman® DigiPrime® 5000 Primer
Description: Primer for digital printingUsage: DigiPrime® 5000 is a print primer which provides excellent adhesion of HP Indigo ElectroInks® to treated films and paper. It adheres well to many..
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | |
|
Struktol TPW 709 Processing Additive
A unique proprietary blend of non-metal internal/external processing aids.Applications: STRUKTOL® TPW 709 has shown excellent results in producing extruded polymer/wood composites with or without..
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | ASTM D792 |
|
Teknor Apex TELCAR® 1050-75 Thermoplastic Elastomer
Information provided by Teknor Apex Company
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | ASTM D792 |
|
Teknor Apex Telcar® TL-1934A BLK 111 Thermoplastic Elastomer
Information Provided by Teknor Apex
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | ISO 1183/1 |
|
A. Schulman FORMION™ FI 342 Ionomer
Information provided by A. Schulman.
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | ASTM D792 |
|
A. Schulman POLYFLAM™ RPP 1360 Non-Halogenated Homopolymer Polypropylene
DescriptionPolyflam® RPP 1360 is a UL 94 V0 rated, non-halogenated homopolymer polypropylene flame retardant compound. Information provided by A. Schulman.
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | ASTM D792 |
|
A. Schulman POLYFORT™ FPP 2067HU UV Stabilized, High Heat Resistant Impact Polypropylene
DescriptionPolyfort® FPP 2067HU is a unique high flow, UV stabilized high heat resistant impact polypropylene available in matched automotive colors. It molds to a fine appearance with good scrat..
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | |
|
Zylog Hipolyene® 8515 TY Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | ISO 1183/1 |
|
A. Schulman FORMION™ FI 342 Ionomer
Information provided by A. Schulman.
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | |
|
Zeon Chemicals Nipol® 1051 Nitrile Elastomer
Nipol 1051 is a copolymer of butadiene and acrylonitrile with very high oil resistance. Sufficient antioxidant is added during manufacture for normal storage conditions.Easy processing version of Ni..
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | ASTM D792 |
|
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman.
|
|||
| Specific Gravity |
1.00
g/cc @Temperature 25.0 °C |
1.00
g/cc @Temperature 77.0 °F |
|
|
Dow Corning FG-10 ANTIFOAM EMULSION
10 percent active, food-grade silicone emulsion designed to control foam in aqueous systems.Information provided by Dow Corning
|
|||
| Specific Gravity |
1.00
g/cc @Temperature 25.0 °C |
1.00
g/cc @Temperature 77.0 °F |
|
|
Dow Corning MOLYKOTE® BG-555 LOW NOISE GREASE
Lithium thickened polyolester greaseInformation provided by Dow Corning
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | ISO 2781 |
|
ELASTO UK Dryflex® 8004-002 Flame Retardant TPE for Extrusion, White, Halogen Free
Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and..
|
|||
| Specific Gravity |
1.00
g/cc @Temperature 25.0 °C |
1.00
g/cc @Temperature 77.0 °F |
|
|
Dow Corning 4 ELECTRICAL INSULATING COMPOUND
Silicone-based compound, moderate consistency. Lubricant suitable for electrical connectors and joints.Information provided by Dow Corning
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | Uncatalyzed, Moldmaster Blue |
|
ACC QM 2128 QSI Quantum Silicones 28 Durometer Condensation Cure Moldmaking Material
QM 2128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch..
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | Uncatalyzed, QM CAT SKIN 30 |
|
ACC QM Skin 30 QSI Quantum Silicones 30 Durometer Condensation Cure moldmaking Material
QM Skin 30 is a two-component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and very low bleed in addition to good shelf-l..
|
|||
| Specific Gravity | 1.00 - 1.10 g/cc | 1.00 - 1.10 g/cc | ASTM D792 |
|
Aaron Industries AAROPRENE® ATPR 1000 50A Elastomeric Compound
AAROPRENE® ATPR 1000 Series Elastomeric CompoundDurometer values may be specified. Color may be specified.
|
|||
| Specific Gravity | 1.00 - 1.10 g/cc | 1.00 - 1.10 g/cc | ASTM D792 |
|
Aaron Industries AAROPRENE® ATPR 1000 60A Elastomeric Compound
AAROPRENE® ATPR 1000 Series Elastomeric CompoundDurometer values may be specified. Color may be specified.
|
|||
| Specific Gravity | >= 1.00 g/cc | >= 1.00 g/cc | |
|
Parker Chomerics CHO-BOND 1053, Part B Silicone Rubber Mixture
Information provided by Chomerics
|
|||
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | ASTM D792 |
|
PolyOne Synprene® IT 37-035 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledUV StabilizedApplications:General PurposeMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First Choic..
|
|||