Buckeye Polymers BP FLEX A6810 BLK Thermoplastic Elastomer SEBS

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE , Styrene-Butadiene
Manufacturer Buckeye Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Buckeye Polymers BP FLEX A6810 BLK Thermoplastic Elastomer SEBS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Information: BP Flex Thermoplastic Elastomers are based on SEBS polymers (Styrene-ethylene/butylene-styrene) providing increased oxidation and weather resistance, higher service temperatures, and increased processing stability.Product Features:Excellent low temperature performanceReprocessableValves - seals, grommets, under hood applicationsSuperior ozone resistanceAppearance: BlackForms: PelletsProcessing Method: Injection MoldingInformation Provided by Buckeye Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.16 - 1.20 g/cc
1.16 - 1.20 g/cc
ASTM D792
Melt Flow 4.0 - 37 g/10 min
4.0 - 37 g/10 min
ASTM D1238
Ash 32 - 39 %
32 - 39 %
ASTM D5630
Mechanical Properties Metric English Comments
Hardness, Shore A 68 - 75
68 - 75
ASTM D2240