Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.65 - 2.15 g/cc | 1.65 - 2.15 g/cc | |
Parker Chomerics CHO-SEAL S6304 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Specific Gravity | 1.65 - 1.75 g/cc | 1.65 - 1.75 g/cc | ISO 1183 |
Raschig Group AMPLA® 7250 melamine-modified polyester Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
PolyOne Edgetek® XP9242701 Polyphenylene Sulfide (PPS) Injection Speed: 50 to 80% Holding Time: 3 to 9 sec Injection Time: 1 to 3 sec Cycle Time: 18 to 70 secInformation provided by PolyOne |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
DuPont Performance Polymers Rynite® RE15022 NC010 PET
(Unverified Data**) Rynite® RE15022 NC010 is a 36% glass reinforced product designed for applications that need high burst strength.Information provided by DuPont Performance Polymers |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | Method A; ASTM D792 |
LNP Thermocomp® UF-1006 FR HS LEX BK8-115 Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Features: Heat Stabilized, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many L.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
PolyOne Edgetek® SF-40GF/000 Polyphenylene Sulfide (PPS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1301-7815 PPS, linear, with carbon fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrically .. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ISO 1183 |
GEHR Plastics PPS-40GF Polyphenylene Sulfide, 40% Glass Fiber The linear polyphenylensulfide belongs to the semi-crystalline materials and offers a very high mechanical capacity, thermal and chemical resistance distinguished at the same time, high dimensional .. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
LG Chemical LUSEP GP2400 PPS+GF40%, General Purpose Feature: Injection Molding, PPS+GF40%, General PurposeApplication: Pump Units, Motor Units, etc.CAS No. 25212-74-2 and 65997-17-3Information provided by LG Chemical |
|||
Specific Gravity | 1.65 - 1.70 g/cc | 1.65 - 1.70 g/cc | ASTM D792 |
Loxim 230 01V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® 865 PBT (Europe-Africa-Middle East) VALOX 865 is a 30% glass fibre reinforced, non blooming flame retardant PBT+PET blend with an excellent surface appearance. Applications: External housings, steam irons, appliance housings and light.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | |
Silberline EternaBrite® Premier 255 EternaBrite® Premier 255 is a fine, very bright, leafing aluminum pigment with excellent opacity and distinctness of image (D.O.I) for solvent based general industrial coatings. This product is s.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® XP-2130A PPS Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® XP-2130A PPS Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
Teknor Apex Fireguard® 910L16-C13-NL Polyvinyl Chloride, Flexible Notes: RoHS Compliant Features: Flame Retardant; Low Smoke Emission Uses: Plenum Cable Jacketing Wire Types: CL2P; CL3P; CMP; FPLP; MPP; OFNP Agency Ratings: NEC Article 725; NEC Article 760; NEC Ar.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
Colorite Polymers CS7566LS Wire and Cable Jacket Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | |
Aremco Glass-Coat™ GC4000 High Temperature Specialty Coatings Glass Glass-enamel, gloss-black coating for stainless steel to 1000°F (538°C) |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | |
Aremco Ceramacoat™ 845-GRY High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, gray coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadiu.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | Film |
Solvay Specialty Polymers Diofan® A610 Polyvinylidene Chloride (PVDC)
(discontinued **) DIOFAN® A610 is a water based dispersion of a polyvinylidene chloride copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances. It features exceptional barrier.. |
|||
Specific Gravity | 1.65 - 1.95 g/cc | 1.65 - 1.95 g/cc | |
Parker Chomerics CHO-SHIELD® 598 A/B Silver-Epoxy Coating Silver-Epoxy Coating. This coating is a two-component, silver bearing, highly conductive epoxy paint designed to provide EMI shielding when applied to a plastic, non-conductive substrate. Used as a .. |
|||
Specific Gravity | 1.65 - 1.80 g/cc | 1.65 - 1.80 g/cc | ISO 1183 |
Raschig Group DECAL® 152CL Phenolic Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet.. |
|||
Specific Gravity | 1.65 - 1.70 g/cc | 1.65 - 1.70 g/cc | ASTM D792 |
Adamas Adalon® 266 PTFE, Mineral/Glass Bubbles Filler Information provided by Adamas, HPM |