Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.57 g/cc | 1.57 g/cc | ASTM D792 |
Ovation Polymers Opnyl OP66GF50 Nylon 66 Nylon 66-Glass reinforced(50%), high tensile strength, stiffness and HDT.Information provided by Ovation Polymers |
|||
Specific Gravity | 1.57 g/cc | 1.57 g/cc | ASTM D792 |
Gharda Chemicals Gafone S S1430SP60 Polysulfone (PS)
(discontinued **) Characteristics: High Temperature Resistance - Tg 189°C Excellent Clarity Excellent Mechanical & Electrical properties Easy to process Very good Hydrolytic Resistance Applications: Elec.. |
|||
Specific Gravity | 1.57 g/cc | 1.57 g/cc | ASTM D792 |
LG Chemical Lupox® NH2306F PBT+GF30% Description: Injection Molding, PBT+GF30%, Halogen Free Flame RetardantApplication: IT/OA, E&E (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Specific Gravity | 1.57 g/cc | 1.57 g/cc | ISO 1183 |
Lanxess Durethan® BKV 50 H EF DUS022 900116 Nylon 6, Glass Fiber Reinforced PA 6, 50% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Specific Gravity | 1.57 g/cc | 1.57 g/cc | ISO 1183 |
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers PA 6, 50% glass fibers, injection molding, heat-ageing stabilized |
|||
Specific Gravity | 1.57 g/cc | 1.57 g/cc | |
Momentive Performance Materials Electro 170 Heat Cured Rubber - High Voltage Insulating Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Specific Gravity | 1.57 g/cc | 1.57 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East) VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Specific Gravity | 1.57 g/cc | 1.57 g/cc | ASTM D792 |
Shinkong Synthetic Fibers Shinite® F202G30 PBT, 30% Glass Filled, Fire Retardant, Halogen Free Information from Shinkong Synthetic Fibers Corp. |
|||
Specific Gravity | 1.57 g/cc | 1.57 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP LCF62E PEEK LNP* THERMOCOMP* LCF62E is a compound based on Polyetheretherketone resin containing 10% Carbon, 30% Glass Fiber fillers. Added features of this material includes: Easy Molding, Electrically Condu.. |
|||
Specific Gravity | 1.57 g/cc | 1.57 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® MKD-1015 PA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.57 g/cc | 1.57 g/cc | ISO 1183/1 |
A. Schulman SCHULAMID® 66 GF50 50% Glass Fiber Reinforced 66 Information provided by A. Schulman. |
|||
Specific Gravity | 1.57 g/cc | 1.57 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White 8153/UV2 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 8153/UV2 is a white/UV masterbatch based in polyethylene. This product has been specifically engineered to provide dispersion and opacity at a competitive cost with good dist.. |
|||
Specific Gravity | 1.57 g/cc | 1.57 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White 8750 Concentrate Based In HDPE DescriptionPOLYBATCH® B8750 is a specialty white masterbatch based in HDPE. This product has been designed to achieve optimum dispersion and excellent letdown mixing in blow molding applications. .. |
|||
Specific Gravity | 1.57 g/cc | 1.57 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White 8153/UV2 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 8153/UV2 is a white/UV masterbatch based in polyethylene. This product has been specifically engineered to provide dispersion and opacity at a competitive cost with good dist.. |
|||
Specific Gravity | 1.57 g/cc | 1.57 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White 8750 Concentrate Based In HDPE DescriptionPOLYBATCH® B8750 is a specialty white masterbatch based in HDPE. This product has been designed to achieve optimum dispersion and excellent letdown mixing in blow molding applications. .. |
|||
Specific Gravity | 1.57 g/cc | 1.57 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Red 5170 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 5170 is a red color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 5170 contains .. |
|||
Specific Gravity | 1.57 g/cc | 1.57 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Red 5170 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 5170 is a red color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 5170 contains .. |
|||
Specific Gravity | 1.57 g/cc | 1.57 g/cc | ASTM D792 |
Clariant Renol PA213G50 Nylon 6, 50% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Specific Gravity | 1.57 - 1.61 g/cc | 1.57 - 1.61 g/cc | ASTM D-792 |
Axiall 01560 Plenum Flexible PVC CAT 5 rated plenum jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.57 g/cc | 1.57 g/cc | ASTM D792 |
Asahi Kasei Thermylon® NSG-240A-C 50% Ceramic and Glass Fiber Reinforced Information provided by Asahi Thermofil |
|||
Specific Gravity | 1.57 g/cc | 1.57 g/cc | uncured |
Atom Adhesives AA-BOND F156 Epoxy Adhesive AA-BOND F156 is a black, solvent free thixotropic epoxy recommended for high quality photographic industry, laminating, production and repair applications where a room temperature cure optically opa.. |