Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Rigid Extrusion 87771 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D-792 |
PlastiComp Complet® LCF40-PEI Polyetherimide, 40% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyetherimide with 40% long carbon fiber reinforcementInformation provided by PlastiC.. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
Solvay Specialty Polymers Cogegum® GFR/360 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 20-8171 Polyphthalamide, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
Kotec Carbotex KGN-30MRA Polycarbonate, Flame Retardant, 30% Glass Fiber Reinforced Features: Glass fiber 30% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E .. |
|||
Specific Gravity | 1.43 - 1.49 g/cc | 1.43 - 1.49 g/cc | ASTM D 792 |
Karina 811-10/9-Y-CRB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.43 g/cc @Temperature 23.0 °C |
1.43 g/cc @Temperature 73.4 °F |
ASTM D792 |
Kingfa JH710 G30 Flame Retardant & 30% Glass Fiber Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc.. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON DEL36 PC LNP* STAT-KON* DEL36 is a compound based on Polycarbonate resin containing 30% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive, Wear Resistant. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | |
Shinil Chemical SHINFLAME PBT Flame Retardant Polymer Connector SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod.. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
Techmer ES Plaslube® J-1/20/TF/20 NAT PA66 |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp RF006PS PA 66 LNP* Thermocomp* RF-1006 EP HS is based on Nylon 6/6 containing Glass Fiber. Characteristics of this grade include Exceptional Processing and Heat Stabilizer.This data was supplied by SABIC-IP for .. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
Teknor Apex HFFR 2003 Polyolefin, Halogen Free Notes: RoHS Compliant Features: Flame Retardant; Halogen Free Uses: Communication Wire Jacketing; Electronic Cable Jacketing; Security Cable Jacketing; Fiber Optic Cable Agency Ratings: IEC 60332-1;.. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
Shinkong Synthetic Fibers Shinite® C501G40 Nylon 6, 40% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D 792 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
Teknor Apex Sinvicomp SRF 2704 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Good Weather Resistance; Good Impact Resistance; Good Processability Uses: Fittings Forms: Pellets Processing Method: Injection MoldingInformation Provided by Te.. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
Teknor Apex Sinvicomp SRP 5602 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Good ProcessabilityUses: Conduit; Piping; Profiles Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
Chase Plastics CP Pryme® PC330GR Polycarbonate (Utility Grade), 30% Glass Fiber Reinforced, Mold Release Information provided by Chase Plastics. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Canyon 10290U/4 Concentrate Based In LLDPE DescriptionPOLYBATCH® 10290U/4 is a canyon color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stabilit.. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Treated Pine 60181U/4 Concentrate Based In LLDPE DescriptionPOLYBATCH® 60181U/4 is a treated pine color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV s.. |
|||
Specific Gravity | 1.43 - 1.47 g/cc | 1.43 - 1.47 g/cc | ASTM D-792 |
Axiall 10801 Wire & Cable Flexible PVC Jacket compound recommended for 80°C maximum service temperature at a minimum wall thickness of 30 mils. UL recognized for 720 hour sunlight resistance.Information provided by Georgia GulfGeorgia .. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D-792 |
Axiall 7055 Rigid PVC, Extrusion Georgia Gulf 7055 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: WeatherabilityChemicalDurabilityEase of ProcessingToughnessInformat.. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
PolyOne Nymax™ GF 1800 43 Natural Nylon 612 with 43% Glass Fiber
(discontinued **) Molded Test Bars: Dry as Molded |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® HFD4413 PC (Europe-Africa-Middle East) Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
PolyOne Edgetek® AM-30GM/15TF Polyphthalamide (PPA), Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |