Shinil Chemical SHINFLAME PBT Flame Retardant Polymer Connector

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Flame Retardant
Manufacturer Shinil Chemical
Trade Name SHINFLAME
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shinil Chemical SHINFLAME PBT Flame Retardant Polymer Connector.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to produce high performance SHINFLAME compound. SHINFLAME compounds comprise halogen or non halogen flame retardant additives in engineering thermoplastics. SHINFLAME provides a wide range of the flame performance (V0, V1, V2, HB etc), mechanical and physical properties to create the application-specific environment.Feature and BenefitsExcellent fire performanceNon halogen FR availableEnvironmentally friendlyRoHS compliance (selected grade)Outstanding mechanical propertiesImproved thermal propertiesEasy processingNon toxicInformation Provided by Shinil Chemical Industry Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 62.3 MPa
9030 psi
Elongation at Break 30 %
30 %
Flexural Strength 117.72 MPa
17074 psi
Flexural Modulus 3.04 GPa
441 ksi
Izod Impact, Notched 0.294 J/cm
0.551 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 164 °C
327 °F
Flammability, UL94 V-0
V-0