PlastiComp Complet® LCF40-PEI Polyetherimide, 40% Long Carbon Fiber Reinforced

Category Polymer , Thermoplastic , Polyetherimide (PEI) , Polyetherimide (PEI), Carbon Fiber Filled
Manufacturer PlastiComp
Trade Name Complēt®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastiComp Complet® LCF40-PEI Polyetherimide, 40% Long Carbon Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyetherimide with 40% long carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D-792
Filler Content 40 %
40 %
Long Carbon Fiber
Mechanical Properties Metric English Comments
Tensile Strength 186 MPa
27000 psi
ASTM D-638
Elongation at Break 1.0 %
1.0 %
ASTM D-638
Tensile Modulus 34.483 GPa
5001.3 ksi
ASTM D-638
Flexural Strength 331 MPa
48000 psi
ASTM D-790
Flexural Modulus 31.034 GPa
4501.1 ksi
ASTM D-790
Izod Impact, Unnotched 6.94 J/cm
13.0 ft-lb/in
ASTM D-4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ASTM D-648