Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.03 g/cc | 1.03 g/cc | ASTM D792 |
Polymax® Maxelast® P3892 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 1.03 g/cc | 1.03 g/cc | ASTM D792 |
Network Polymers MS 175 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Specific Gravity | 1.03 g/cc | 1.03 g/cc | ASTM D-792 |
Chevron Phillips MA9545 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Medical containersTamper resistant closuresAudio cassette cases and media packagingFeatures:Information provided by Chevron PhillipsThe Chevron P.. |
|||
Specific Gravity | 1.03 g/cc | 1.03 g/cc | |
TSE Industries Millathane® 26 Millable Polyether Urethane for Food Contact Applications Millathane 26 is a polyether polyurethane rubber compliant with the United States Code of Federal Regulations*, Title 21 parts 177.1680 and 177.2600. This polyurethane rubber is designed for food co.. |
|||
Specific Gravity | 1.03 g/cc | 1.03 g/cc | ASTM D792 |
LG Chemical ALPHALAC SH860 HIPS Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Refrigerator Inner LinerCAS No. 9003-55-8Information provided by LG Chemical |
|||
Specific Gravity | 1.03 g/cc | 1.03 g/cc | ASTM D792 |
LG Chemical HIPS 501S PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Food Holder, Food Container, Plastic Toy, Sheet or Film of Yot ReceptacleCAS: 9003-55-8Information provi.. |
|||
Specific Gravity | 1.03 g/cc | 1.03 g/cc | ASTM D792 |
GRECO ISOPAK 547M ABS Resin Metal Plating GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Michelman® Micryl™ 766R Water resistant coating Description: General purpose water resistant coatingUsage: Micryl™ 766R is a water and grease resistant coating that can also function as a heat resistant gloss overprint. In such applications,.. |
|||
Specific Gravity | 1.03 g/cc | 1.03 g/cc | ASTM D792 |
Mitsui APELâ„¢ APL6011T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Specific Gravity | 1.03 g/cc | 1.03 g/cc | ASTM 792 |
Multibase Multi-Flex® A 8502 LC UV RXF/YYWA Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Specific Gravity | 1.03 g/cc | 1.03 g/cc | |
Struktol VLB 602 LUBRICANT ADDITIVE FOR PVC AND POLYMER PROCESSING Blend of fatty acid esters.Applications: STRUKTOL® VLB-602 is a very compatible complex ester lubricant. It has noted performance in clear calendared PVC sheet. It also has application in clear e.. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Samsung Cheil Industries Starex® SF-100H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Samsung Cheil Industries Starex® SF-300H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Samsung Cheil Industries Starex® SG-501 Expandable Polystyrene (EPS) High Expansion Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.03 g/cc | 1.03 g/cc | ASTM D792 |
Samsung Cheil Industries Starex® SL-0110 ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.03 g/cc | 1.03 g/cc | ASTM D792 |
Teknor Apex Sinpolene GPP5620 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Glass Fiber Reinforcement, 20% Filler by Weight Features: Good Dimensional Stability; High Heat Resistance; .. |
|||
Specific Gravity | 1.03 g/cc | 1.03 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 1285 Glass Fiber-Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP1285 is a 20% glass fiber-reinforced copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 1.03 g/cc | 1.03 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Deep Red 50389 Concentrate Based In Linear Low-Density Polyethylene DescriptionPOLYBATCH® 50389 is a deep red color concentrate based in linear low density polyethylene. This product was formulated to offer color in polyethylene film applications. POLYBATCH® 503.. |
|||
Specific Gravity | 1.03 g/cc | 1.03 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 1285H Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1285H is a 20% glass reinforced copolymer polypropylene compound. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Specific Gravity | 1.03 g/cc @Temperature 25.0 °C |
1.03 g/cc @Temperature 77.0 °F |
|
Dow Corning 752 ADHESIVE/SEALANT General purpose silicone adhesive/sealantInformation provided by Dow Corning |
|||
Specific Gravity | 1.03 g/cc @Temperature 25.0 °C |
1.03 g/cc @Temperature 77.0 °F |
|
Dow Corning SYL-OFF® 7210 RELEASE MODIFIER Syl-Off® 7210 Release Modifier is a 60% active solids, pre-catalysed, release modifier. General purpose release modifier recommeded for use with Syl-Off® Solvent based, platinum catalysed release .. |
|||
Specific Gravity | 1.03 g/cc | 1.03 g/cc | |
Chesterton OPTICOOL™ 462 Lubrication Description: OPTICOOL 462 is a unique blend of high performance additives and superior oil-based lubrication. OPTICOOL 462 offers cost effective dilutions corrosion inhibition, extreme pressure resi.. |
|||
Specific Gravity | 1.03 g/cc | 1.03 g/cc | ASTM D-792 |
Chevron Phillips MB3150 Crystal Polystyrene High heat crystal polystyrene.Applications:Compact disc jewel boxesConsumer containers, vials, jars, etc.Desk organizersAudio cassettesFeatures:Fast cycling due to high heat distortionHigh Vicat sof.. |
|||
Specific Gravity | 1.03 g/cc | 1.03 g/cc | ASTM D792 |
Diamond Polymers SBS 2160 Clear Styrene Butadiene Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Specific Gravity | 1.03 g/cc @Temperature 25.0 °C |
1.03 g/cc @Temperature 77.0 °F |
|
Dow Corning 2-3902 Antifoam Compound 100% active silicone fluid containing a suspension of finely powdered silica to enhance its defoaming efficiency.Information provided by Dow Corning |
|||
Specific Gravity | 1.03 g/cc @Temperature 25.0 °C |
1.03 g/cc @Temperature 77.0 °F |
|
Dow Corning 43 Paperaid Dow Corning® Paperaid 43 is 100% solids silicone polyether. Suitable as antifoam in the production of rosin size.Information provided by Dow Corning |
|||
Specific Gravity | 1.03 g/cc | 1.03 g/cc | Uncatalyzed, QM CAT 135 |
ACC QM 135 QSI Quantum Silicones 35 Durometer Condensation Cured Moldmaking Material QM 135 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent cho.. |
|||
Specific Gravity | 1.03 g/cc | 1.03 g/cc | ASTM D792 |
LTL Color Compounds ColorFast® GPA300X ABS Extrusion grade, high impact, high gloss ABSAll information provided by LTL Color Compounders, Inc. |