Dow Corning 2-3902 Antifoam Compound

Category Polymer , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 2-3902 Antifoam Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
100% active silicone fluid containing a suspension of finely powdered silica to enhance its defoaming efficiency.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc

@Temperature 25.0 °C
1.03 g/cc

@Temperature 77.0 °F
Viscosity Measure 25300 - 29600 cSt
25300 - 29600 cSt
Kinetic/Kinematic