Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D792 |
S&E Specialty Polymers GA-509ORLT PVC Application: Lead free, flame retardant UV and oil resistant PVC jacketing compound with superior low temperature properties.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D792 |
S&E Specialty Polymers TufFlex™ GTPE-2272 TPE Compound Application: A 105°C flexible, oil resistant, flame retardant TPE jacketing material designed for SJEO applications.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.10 - 1.30 g/cc | 1.10 - 1.30 g/cc | |
PolyChem Alloy PolyGard 3005R PolyFoam decomposes when heated to create a uniform microcellular structure. It can be used in extrusion and injection molding processes to reduce weight in parts without adversely affecting the ph.. |
|||
Specific Gravity | 0.900 - 1.30 g/cc | 0.900 - 1.30 g/cc | |
Parker Chomerics CHO-SHIELD® 2056 Conductive Coating CHO-SHIELD® 2054 silver-plated-copper filled commercial-grade coating proved high levels of EMI shielding effectiveness, abrasion resistance and excellent adhesion on a variety of materials used fo.. |
|||
Specific Gravity | 1.20 - 1.30 g/cc | 1.20 - 1.30 g/cc | |
PolyChem Alloy AquaGard™ 3004M AquaGard products are designed to improve the flame retardency of polyolefins without the use of halogen additives, such as bromine or chlorine. AquaGard products are available in a polyethylene .. |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D 792 |
Karina 701D25-1-A-IS Natural PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D 792 |
Karina 722-48/1-A-IS Black PVC Compound Heavy metal free PVC compound recommended for extrusion of automobile profilesInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | NBR NM-IEC 60811-1-3 |
Karina 771-48/1-BY-IS-BZ Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D 792 |
Karina 800-10/10-IS White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.26 - 1.30 g/cc | 1.26 - 1.30 g/cc | ASTM D 792 |
Karina 800D48/1-A-IS-BZ Black PVC Compound Heavy metal free PVC compound recommended for injection and extrusion of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D 792 |
Karina 920D32/91 Orange PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | NBR NM-IEC 60811-1-3 |
Karina E 42/183-FC-LMP Red Color Concentrate for PVC Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes.Important con.. |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D 792 |
Karina E 42/261-GEN Dark Red MBATCH (SP31543) for PVC Recommended usage from 2% to 3% on crystal PVC compoundInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D 792 |
Karina E 57/200-D-AT-IS-SD Clear PVC Compound PVC compound recommended for shrink films.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D 792 |
Karina E 680D18/487-B-IS Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D 792 |
Karina E 680D35/1-B-IS Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D 792 |
Karina 57/200-D-AT-IS-SD Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D 792 |
Karina E 57/201-D-IS-SD Compound PVC Crystal Clear/crystal PVC compound specially developed for skin films.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.27 - 1.30 g/cc | 1.27 - 1.30 g/cc | ASTM D792 |
Spartech Royalite R47 PVC Alloy Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |
|||
Specific Gravity | 1.27 - 1.30 g/cc | 1.27 - 1.30 g/cc | ASTM D792 |
Spartech Royalite R522 PVC Alloy Aircraft Grade Sheet Description: Aircraft Grade SheetInformation provided by Spartech. |
|||
Specific Gravity | 1.26 - 1.30 g/cc | 1.26 - 1.30 g/cc | ASTM D-792 |
Axiall 8560 Moldings & Extrusions Flexible PVC A clear, semi-rigid extrusion or molding grade compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.26 - 1.30 g/cc | 1.26 - 1.30 g/cc | ASTM D-792 |
Axiall EX1188B Wire & Cable Flexible PVC UL 360 jacket compound. 105°C air; 60°C oil.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.26 - 1.30 g/cc | 1.26 - 1.30 g/cc | ASTM D-792 |
Axiall 11470 Wire & Cable Flexible PVC Highly flame retardant clear compound. Recommended as jacket in PVC/PVC VW-1 constructions.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.26 - 1.30 g/cc | 1.26 - 1.30 g/cc | ASTM D-792 |
Axiall 19740 Wire & Cable Flexible PVC Non-lead stabilized, 105°C rated insulation compound with excellent low temperature properties. Suitable for use in Class 43 applications. Also suitable for injection molding applications.Informa.. |
|||
Specific Gravity | 0.900 - 1.30 g/cc | 0.900 - 1.30 g/cc | |
Parker Chomerics CHO-SHIELD® 2052 Conductive Coating CHO-SHIELD® 2052 silver-plated-copper filled commercial-grade coating proved high levels of EMI shielding effectiveness, abrasion resistance and excellent adhesion on a variety of materials used fo.. |
|||
Specific Gravity | 1.26 - 1.30 g/cc | 1.26 - 1.30 g/cc | ASTM D-792 |
Axiall 8681 Moldings & Extrusions Flexible PVC General purpose, elastomeric vinyl compound well suited for co-extrusion with rigid PVC.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.26 - 1.30 g/cc | 1.26 - 1.30 g/cc | NBR NM-IEC 60811-1-3 |
Karina 02/223-G Yellow Color Concentrate for PVC Color concentrate recommended for application in PVC compounds for general purposes injection. Recommended to use 2%.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.26 - 1.30 g/cc | 1.26 - 1.30 g/cc | ASTM D 792 |
Karina CAK 55-48/1 Black PVC Compound Reclaimed PVC compound recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.26 - 1.30 g/cc | 1.26 - 1.30 g/cc | ASTM D-792 |
Axiall 18650 Moldings & Extrusions Flexible PVC General purpose compound recommended for 105C applications. Well suited for 105C molding and general purpose extrusions.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in.. |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D 792 |
Karina E 57/200-D-AT-IS-SI-SD Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |