Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D792 |
Quantum PPSU Information provided by Quantum Advanced Engineering Plastics |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ASTM D792 |
PTS PBT-1090 PBT Resin Information provided by PTS LLC. |
|||
Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D792 |
PolyOne FireCon™ CPE 30-11 REV 2 Polyethylene, Chlorinated (CPE) CPE-30-11 REV 2 is a heavy duty thermoplastic jacket for power and control cables. It is suitable for VW1 and tray fire rated applications. CPE-30-11 REV 2 offers high tensile and superior fluid res.. |
|||
Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D792 |
Ravago Manufacturing Americas Enviramid™ N1320HL BK Post Consumer Recycle Nylon 66, 20% Glass Filled Heat Stabilized, Lubricated, Black, and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D792 |
PolyOne Edgetek® MLS-10GF/000 Polysulfone Alloy - 10% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Specific Gravity | 1.29 g/cc | 1.29 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-8059 PEEK, lubricant modified, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Specific Gravity | 1.29 - 1.35 g/cc | 1.29 - 1.35 g/cc | ASTM D 792 |
Karina 36/19-FC-LMP (SDB) Brown Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D792 |
MRC Polymers NAXALOYâ„¢ 793A3 GF10 PC and Polyester Blend, 10% Glass Fiber Filled 793 GF10 is available in natural and custom colors, internal and external lubricants, UV stabilizer and other modifications.Information provided by MRC Polymers Inc. |
|||
Specific Gravity | 1.29 - 1.35 g/cc | 1.29 - 1.35 g/cc | ASTM D 792 |
Karina 800D10/7-A-IS White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON DE002 PC (Asia Pacific) LNP* Stat-Kon* DE002 is a Polycarbonate containing Carbon Fiber. |
|||
Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D 792 |
SABIC Innovative Plastics Valox® VAC3001 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® NH-1150HH PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® GC-1150 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® NH-1150HH PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF004XXH PA 66 LNP THERMOCOMP* RF004XXH is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM AUT210 PEI (Asia Pacific) Transparent Polyetherimide (Tg 227 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature o.. |
|||
Specific Gravity | 1.29 g/cc | 1.29 g/cc | foam molded; ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM4025 PPE+HIPS (Europe-Africa-Middle East) LNP* Thermocomp* Noryl_FM4025 compound is GR/MR 40%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness. |
|||
Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL GFN3 PPE+PS PPE+PS blend. 30% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui.. |
|||
Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D792 |
Teknor Apex Telcar® TL-1140D BLK Thermoplastic Elastomer Uses: Automotive Applications; Automotive Interior Parts; Blow Molding Applications; Carpet Backing; General Purpose; Grommets; Weatherstripping Forms: Pellets Processing Method: Extrusion; Injectio.. |
|||
Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D792 |
Teknor Apex Vidux® CV-92-A5008A-91 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Features: Antistatic; Conductive; Electromagnetic Shielding (EMI); Non-DEHP Plasticizer; Ethylene Oxide Sterilizable; Radio Frequency Shielding (RFI) Uses: Coating Applications.. |
|||
Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D-792 |
Axiall CL-7049 Rigid PVC, Molding Georgia Gulf CL-7049 is a clear, high impact vinyl compound formulated for medical and food contact uses.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.29 g/cc | 1.29 g/cc | Laminate; ASTM D792 |
Azdel Plus C507-B01 50% Chopped Fiber Mat / PP Resin Matrix (Mineral filled) AZDEL® C507-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat and mineral filler contained within a polypropylene resin matrix. This composite material featu.. |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ISO 1183 |
BLUESTAR PBT 1100A Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ASTM D-792 |
Axiall 21572 Coax & Telecom Flexible PVC Semi-rigid non-lead stabilized insulation compound designed for data communication riser cable applications. Maximum 60°C service temperature rating.Information provided by Georgia GulfGeorgia Gul.. |