Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.024 - 0.028 cm/cm | 0.024 - 0.028 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP FL004 PE (Europe-Africa-Middle East) LNP* Lubricomp* FL004 is a compound based on Polyethylene resin containing PTFE. |
|||
Linear Mold Shrinkage, Flow | 0.024 cm/cm @Time 86400 sec |
0.024 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP FX04491H PE LNP LUBRICOMP* FX04491H is a compound based on Polyethylene resin containing Proprietary Fillers. Added features of this material include: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.024 cm/cm @Time 86400 sec |
0.024 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KI001XXJ Acetal LNP* LUBRICOMP* KI001XXJ is a compound based on Acetal containing 2% Silicone. Added features of this grade include: Wear Resistant, Healthcare. |
|||
Linear Mold Shrinkage, Flow | 0.024 - 0.027 cm/cm @Thickness 3.20 mm |
0.024 - 0.027 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 337 PBT Low temperature impact PBT. Automotive applications: underhood power distribution boxes and covers. |
|||
Linear Mold Shrinkage, Flow | 0.024 cm/cm | 0.024 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific) LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Linear Mold Shrinkage, Flow | 0.024 cm/cm @Time 86400 sec |
0.024 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific) LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Linear Mold Shrinkage, Flow | 0.024 - 0.028 cm/cm | 0.024 - 0.028 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1668-BK1 High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.024 - 0.030 cm/cm @Thickness 4.00 mm |
0.024 - 0.030 in/in @Thickness 0.157 in |
E2P method |
Eurostar Star L PA66 D61 PA66, Injection Molded Star L PA66 D51 is a PTFE/Silicone Oil Lubricated, Unreinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.024 - 0.027 cm/cm @Thickness 4.00 mm |
0.024 - 0.027 in/in @Thickness 0.157 in |
E2P method |
Eurostar Star L POM D84 POM, Injection Molded Star L POM D84 is a PTFE/Proprietary Additive Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.024 cm/cm | 0.024 in/in | ISO 294-4 |
Barlog Plastics KEBAFLEX SG 50 A.1 black TPE-S, Shore A50, black TPE-SInformation provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Flow | 0.024 cm/cm | 0.024 in/in | ISO 294-4 |
Barlog Plastics KEBAFLEX SG 65 A.01 TPE-S, Shore A65, natural TPE-SInformation provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Flow | 0.024 cm/cm | 0.024 in/in | ISO 294-4 |
Barlog Plastics KEBAFLEX SG 60 A.01 black TPE-S, Shore A60, black TPE-SInformation provided by BARLOG plastics GmbH. |