Barlog Plastics KEBAFLEX SG 65 A.01 TPE-S, Shore A65, natural

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Barlog Plastics
Trade Name KEBAFLEX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBAFLEX SG 65 A.01 TPE-S, Shore A65, natural.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TPE-SInformation provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.024 cm/cm
0.024 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
Tensile Strength at Break 7.00 MPa
1020 psi
ISO 527-1
Elongation at Break 660 %
660 %
ISO 527-1
Descriptive Properties Value Comments
Resin Type TPE-S