Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible A75G0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm @Thickness 2.00 mm |
0.019 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® 511DP BK402 Acetal Homopolymer
(Unverified Data**) Delrin® 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided.. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm @Thickness 2.00 mm |
0.019 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG511DP is a medium viscosity acetal homopolymer, with improved thermal stability and modifications for more precise molding. It has been developed for consideration into applications such .. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm | 0.019 in/in | 150x105x3, 260°C / MT 80°C; 500 bar; acc. ISO 2577 |
Lanxess Pocan® DP 7318 000000 PBT, 17% Pigment PBT, 17% white pigments, injection molding, improved light reflection, low tendency to warpInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm | 0.019 in/in | |
Solvay TECHNYL® A 238 Black 21 N PA66, DRY Description: Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 238 offers excellent .. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm | 0.019 in/in | |
Solvay TECHNYL® A 402 Natural FA PA66, DRY Description: Unreinforced polyamide PA66, very high viscosity, for extrusion.Available in: Europe and North AmericaProduct Applications: TECHNYL® A 402 NATURAL FA offers three main advantages: hi.. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm | 0.019 in/in | |
Solvay TECHNYL® A 402H1 Natural PA66, DRY Description: TECHNYL® A 402H1 is an unreinforced polyamide 66, very high viscosity, heat stabilized, for extrusion and injection molding. This product is available in natural color.Benefits: The .. |
|||
Linear Mold Shrinkage, Flow | 0.019 - 0.021 cm/cm @Thickness 3.20 mm |
0.019 - 0.021 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 305 PBT PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 1450-1850. |
|||
Linear Mold Shrinkage, Flow | 0.019 - 0.021 cm/cm @Thickness 3.20 mm |
0.019 - 0.021 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 309 PBT PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 3500-4500. Available in Natural (1001) only. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm @Thickness 3.17 mm |
0.019 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PP 0096 S2 LE Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.019 - 0.021 cm/cm | 0.019 - 0.021 in/in | SABIC Method |
SABIC Innovative Plastics LNP Thermotuf PX06093 PA 6 (Europe-Africa-Middle East) LNP* THERMOTUF* PX06093 is a compound based on PA 6 resin containing Impact Modifier. Added features include: High Impact, UV-Stabilized, Laser Marking Grade.This data was supplied by SABIC-IP for t.. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm | 0.019 in/in | |
Solvay TECHNYL® 27010ST PA66, DRY Description: Polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2710ST is used in all sector of.. |
|||
Linear Mold Shrinkage, Flow | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1606-N Impact Modified Nylon 66 Description: Impact Modified Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1627-GY1 High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® FGS600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Food Contact Applications Crastin FGS600F40 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for injection .. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 511DP BK402 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s.. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG311DP is a medium-high viscosity acetal homopolymer with improved thermal stability and modificati.. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm @Thickness 1.90 mm |
0.019 in/in @Thickness 0.0748 in |
E2P method |
Eurostar Starpylen MB006SU PP, Glass Bead Filled, Injection Molding Resin Starpylen MB006SU is a Glass Bead Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Hytrel® HTR8730 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Viscosity Polyester Elastomer with Excellent Mechanical Properties at Elevated Temperatures Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm | 0.019 in/in | Eurotec |
Eurotec® Tecoform® PO20 NL RM POM, MoS2 modified, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm | 0.019 in/in | ISO 2577 |
BASF Ultraform® N2640 Z2 POM + PUR Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.Information provided by BAS.. |
|||
Linear Mold Shrinkage, Flow | 0.019 cm/cm @Thickness 2.00 mm |
0.019 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® 911DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided by.. |