Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0075 cm/cm
0.0075 in/in
ASTM D955
DuPont Bexloy® AXW504BK Modified Ionomer Resin  (discontinued **)
A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont.
Linear Mold Shrinkage, Flow 0.0075 cm/cm
0.0075 in/in
ASTM D955
DuPont Bexloy® AXW602NC010 3% Glass Reinforced, Heat Stabilized Modified Ionomer Resin  (discontinued **)
A 3% glass reinforced, heat stabilized modified ionomer resin engineered for injection molded interior automotive applications.Availability: North AmericaInformation provided by DuPont.
Linear Mold Shrinkage, Flow 0.0075 cm/cm
0.0075 in/in
Injection molding; ISO 2577
Hexion Bakelite™ PF 2400 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof, UL Listed  (disc
Phenolic molding compound, inorganically/organically filled, average heat resistance, increased dimensional stability, dish washer proof, UL listed molding compound 1.5 mm/V-0 (ALL).Application area..
Linear Mold Shrinkage, Flow 0.0075 cm/cm
0.0075 in/in
Injection molding; ISO 2577
Hexion Bakelite™ PF 2535 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof  (discontinued **
Phenolic molding compound, inorganically/organically filled, average heat resistant, steam resistant, dish washer proof, high surface quality.Application areas: Fittings for ovens and dishwashers, t..
Linear Mold Shrinkage, Flow 0.0075 cm/cm
0.0075 in/in
Injection molding; ISO 2577
Hexion Bakelite™ X65 Phenolic Formaldehyde Resin, UL Listed  (discontinued **)
Phenolic molding compound, inorganically/organically filled, good heat-resistance and dimensional stability, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Oven strips.Information..
Linear Mold Shrinkage, Flow 0.0075 - 0.010 cm/cm
0.0075 - 0.010 in/in
LATI Latene® 7H2W T-V0 PP Homopolymer, Mineral Reinforced, Heat Stabilized, Flame Retardant
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardantsAvailability: Africa & Middle East; Asia Pacif..
Linear Mold Shrinkage, Flow 0.0075 - 0.0095 cm/cm
0.0075 - 0.0095 in/in
LATI Latene® 7H2W T-V0E PP Homopolymer, Mineral Reinforced, Heat Stabilized, Flame Retardant
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle..
Linear Mold Shrinkage, Flow 0.0075 - 0.0095 cm/cm
0.0075 - 0.0095 in/in
LATI Lapex A PES
Polyether Sulfone (PES). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInf..
Linear Mold Shrinkage, Flow 0.0075 - 0.0125 cm/cm
0.0075 - 0.0125 in/in
LATI Laticonther 47/1 CP/80 PP Copolymer
High thermal conductivity product based on Polypropylene copolymer (PPc). Special filler. Extrusion and molding injection grade.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ..
Linear Mold Shrinkage, Flow 0.0075 - 0.0095 cm/cm
0.0075 - 0.0095 in/in
LATI Latigray 82-02 CX/80 PA 12
Radiopaque compound based on Polyamide 12 (PA12). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria..
Linear Mold Shrinkage, Flow 0.0075 cm/cm

@Thickness 3.17 mm
0.0075 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES HiFill FR® PA4/6 GF15 FR HS L 15% Glass Filled (Conditioned)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat St..
Linear Mold Shrinkage, Flow 0.0075 cm/cm

@Thickness 3.17 mm
0.0075 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES Plastiblend® TPX-HTN-000AB 15% Glass Filled
Availability: North AmericaForms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: High Heat ResistanceInformation provided by TP Composites, Inc.
Linear Mold Shrinkage, Flow 0.0075 cm/cm

@Thickness 3.17 mm
0.0075 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES HiFill FR® PA4/6 GF15 FR HS L 15% Glass Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat St..
Linear Mold Shrinkage, Flow 0.0075 cm/cm
0.0075 in/in
Solvay TECHNYL® 52G1MX 25 Grey 7035 PA6, DRY
Description: Flame retardant polyamide PA6 reinforced with mineral filler for injection molding, also suitable for thin wall parts.Available in: Asia Pacific, Europe, Latin America and North America..
Linear Mold Shrinkage, Flow 0.0075 - 0.0105 cm/cm
0.0075 - 0.0105 in/in
ISO DIS 294-4
Wellman Wellamid® GB1430-N 33% Glass Bubble Filled, Low Density Nylon 66
Description: Glass Bubble Filled, Low Density Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Flow 0.0075 - 0.0105 cm/cm
0.0075 - 0.0105 in/in
ISO DIS 294-4
Wellman Wellamid® T512-BK 15% Talc/Glass Reinforced, Dimensionally Stable Grade Nylon 6
Description: Talc/Glass Reinforced, Dimensionally Stable Grade Nylon 6Information provided by Wellman.
Linear Mold Shrinkage, Flow 0.0075 cm/cm

@Thickness 2.00 mm
0.0075 in/in

@Thickness 0.0787 in
60x60x2 mm; ISO 294-4
Covestro Apec® 1603 High-Heat Polycarbonate
This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along..
Linear Mold Shrinkage, Flow 0.0075 cm/cm
0.0075 in/in
ASTM D955
DuPont Bexloy® AXW502NC010 Modified Ionomer Resin  (discontinued **)
A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont.
Linear Mold Shrinkage, Flow 0.0075 cm/cm
0.0075 in/in
48 hrs @ 23°C, flow; SABIC Method
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1030 PP
SABIC® PPcompound 19T1030 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding applications...
Linear Mold Shrinkage, Flow 0.0075 cm/cm
0.0075 in/in
ASTM D955
DuPont Bexloy® AXW604BK 3% Glass Reinforced, Heat Stabilized Modified Ionomer Resin  (discontinued **)
A 3% glass reinforced, heat stabilized modified ionomer resin engineered for injection molded interior automotive applications.Availability: North AmericaInformation provided by DuPont.
Linear Mold Shrinkage, Flow 0.0075 - 0.0115 cm/cm
0.0075 - 0.0115 in/in
LATI Latilub 88/10-10T Y/10 PEEK, 10% Aramid Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati..