Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | ASTM D955 |
PolyOne Stat-Tech™ AS-13CF/000 Black Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® JK2000 PC+ABS (Asia Pacific) Lexan* JK2000 compound is a glass reinforced, non-Br and non-Cl FR polycarbonate blends designed for thinwall molding applications. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0025 cm/cm | 0.00050 - 0.0025 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics LNP Lubricomp DEL34 PC (Europe-Africa-Middle East) LNP* Lubricomp* DEL34 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP f.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm | 0.00050 - 0.0015 in/in | Solvay Test |
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, at Equilibrium (65% RH)
(discontin The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 1200-22 Polycarbonate Resin Description: LUPOY PC 1200-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 1300-15 Polycarbonate Resin Description: LUPOY PC 1300-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 1301-12 Polycarbonate Resin Description: LUPOY PC 1301-12 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 1301EP30 Polycarbonate Resin Description: LUPOY PC 1301EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 3010-10 Polycarbonate Resin Description: LUPOY PC 3010-10 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 cm/cm | 0.00050 in/in | |
Kuraray Genestarâ„¢ GW1458HF Nylon, 45% Glass Filled Low Warpage, High Flow HB grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 1303-10 Polycarbonate Resin Description: LUPOY PC 1303-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 3010-30 Polycarbonate Resin Description: LUPOY PC 3010-30 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 cm/cm | 0.00050 in/in | Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4 |
Lanxess Durethan® BKV 30 H2.0 EF DUS029 901510 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.00050 cm/cm | 0.00050 in/in | Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4 |
Lanxess Durethan® BKV 35 H3.0 000000 Nylon 6, Glass Fiber Reinforced PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4 |
Lanxess Durethan® ECO BV 35 H2 900500 Nylon 6, 35% Glass Fiber PA 6, 35% glass fibers, injection molding, heat-ageing stabilized, contains 30% pre-consumer recycled materialInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0025 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0025 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1530A PC LNP* Lubricomp* Lexan_LF1530A compound is a 30% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm | 0.00050 - 0.0015 in/in | SABIC Method |
SABIC Innovative Plastics LNP Lubricomp UCL36AS PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UCL36AS is a compound based on Polyphthalamide resin containing Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive, Heat Stabilized.This data .. |
|||
Linear Mold Shrinkage, Flow | 0.00050 cm/cm @Thickness 3.17 mm |
0.00050 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® ABS GF50 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.00050 cm/cm @Thickness 3.17 mm |
0.00050 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® ABS GF60 LE 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm @Time 86400 sec |
0.00050 - 0.0015 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DX13320C PC COPOLYMER (Asia Pacific) LNP* Statkon DX13320C is ultra clean polycarbonate/carbon fiber compound with high modulus, good flow ability, easy mold release, and high level of cleanliness for the most demanding application. A .. |
|||
Linear Mold Shrinkage, Flow | 0.00050 cm/cm @Thickness 3.17 mm |
0.00050 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® ASA GF15 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: UV StabilizerFeatures: Good UV ResistanceInformation provided by TP Composites.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Lexan_LCF1506 PC (Europe-Africa-Middle East) LNP* Stat-kon* Lexan_LCF1506 is a 15% carbon fiber, 6% PTFE reinforced polycarbonate. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC1010 PPE+PS LNP* Stat-kon* Noryl_HMC1010 compound is a 10% Carbon fiber reinforced. Static dissipative. Nonbrominated, nonchlor- nated flame retardant system. UL94 V-1 rated. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC3008A PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* Noryl_HMC3008A compound is a 30% glass/mineral/carbon fiber reinforced resin; static dissipative; 250F (120C) HDT. Tight tolerance molding. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0025 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0025 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK5030 PC (Asia Pacific) Glass reinforced. Flame retardant. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm | 0.00050 - 0.0015 in/in | Solvay Test |
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | ASTM D955 |
PolyOne Stat-Tech™ NJ-20CF/000 Black Polyamide 12 (Nylon 12) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 cm/cm @Time 86400 sec |
0.00050 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON NV008E PC+ABS LNP* VERTON* NV008E is a compound based on PC+ABS resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding. Structural. |