Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.010 - 0.015 cm/cm | 0.010 - 0.015 in/in | ASTM D955 |
PolyOne LubriOne™ NN-000/10T Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.015 cm/cm | 0.010 - 0.015 in/in | ASTM D955 |
PolyOne Versollan™ RU 2205-1 Thermoplastic Elastomer (TPE) Versollan™ RU 2205-1 is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performa.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.015 cm/cm | 0.010 - 0.015 in/in | ASTM D955 |
PolyOne Versollan™ RU 2205-9 Thermoplastic Elastomer (TPE) Versollan™ RU 2205-9 is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performa.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.015 cm/cm @Thickness 4.00 mm, Temperature 23.0 °C |
0.010 - 0.015 in/in @Thickness 0.157 in, Temperature 73.4 °F |
Injection Molded, Bergmann Method; ASTM D955 |
PolyOne Bergamid™ B70 GK/Mi30 BK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.015 cm/cm | 0.0090 - 0.015 in/in | ASTM D955 |
PolyOne Dynaflex™ G7960-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7960-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.015 cm/cm | 0.0090 - 0.015 in/in | ASTM D955 |
PolyOne Dynaflex™ G7660-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7660-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible B80MB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.015 cm/cm @Thickness 3.20 mm |
0.012 - 0.015 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL HM3207 PP+MF20%, High Stiffness Description: Injection Molding, PP+MF20%, Good Weatherability, High StiffnessApplication: Automotive Interior Parts CAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.015 cm/cm | 0.010 - 0.015 in/in | |
LATI Latigray 52/11-01 CX/70 PP Homopolymer Radiopaque compound based on Polypropylene homopolymer (PPh). Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | |
LATI Latigray 53/22-01 CX/70 PP Homopolymer, Impact Modified Radiopaque compound based on Polypropylene homopolymer (PPh), impact modified. Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | |
LATI Latilub 45/7-20T HDPE, PTFE Reinforced Self-lubricating product based on High density polyethylene (HD-PE). PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm @Time 86400 sec |
0.011 - 0.015 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOTUF R1000I PA 66 High Impact Nylon 66 compound containing Impact Modifier. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm @Time 86400 sec |
0.011 - 0.015 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOTUF R1000I PA 66 (Asia Pacific) High Impact Nylon 66 compound containing Impact Modifier. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.015 cm/cm | 0.010 - 0.015 in/in | SABIC Method |
SABIC Innovative Plastics LNP Thermotuf R1000IX2 PA6.6 (Europe-Africa-Middle East) LNP* THERMOTUF* R1000IX2 is a compound based on PA 66 resin, containing Impact Modifier. Added features include: High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | annealed 130C 1hr; ASTM D955 |
SABIC Innovative Plastics NORYL GTX GTX902 PPE+PS+PA Unreinforced. Excellent chemical resistance and paintability. 312F (155C) HDT. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | annealed 130C 1hr; ASTM D955 |
SABIC Innovative Plastics NORYL GTX GTX902 PPE+PS+PA (Asia Pacific) Unreinforced. Excellent chemical resistance and paintability. 312F (155C) HDT. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.015 cm/cm @Thickness 3.20 mm |
0.013 - 0.015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Asia Pacific) Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | DIS 294-4 |
Wellman Wellamid® 42LN2-N Nylon 6, General Purpose All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | ISO DIS 294-4 |
Wellman Wellamid® GS40-66 22L-Bk1 40% Glass Sphere Filled Nylon 66 Description: Glass Sphere Filled Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | on Tensile Bar; E2P method |
Eurostar Staramide B28 PA6, Injection Molded Staramide B28 is an Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | on Tensile Bar; E2P method |
Eurostar Staramide B40 PA6, Extrusion Staramide B40 is High Viscosity, Unreinforced Polyamide 6, Extrusion ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.015 cm/cm | 0.010 - 0.015 in/in | on Tensile Bar; E2P method |
Eurostar Staramide BS6 PA6, 30% Glass Bead Filled, Injection Molded Staramide BS6 is a 30% Glass Bead Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm | 0.011 - 0.015 in/in | on Tensile Bar; E2P method |
Eurostar Staramide RB006S PA66, 30% Glass Bead Filled, Injection Molded Staramide RB006S is a 30% Glass Bead Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 30K S3)Information provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.015 cm/cm | 0.0080 - 0.015 in/in | on Tensile Bar; ISO 294 |
Eurostar Starflam R10002E PA66/6, Injection Molded Starflam R10002E is a Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 66/Polyamide 6 Injection Molding Resin (also known as R1000Z220EM)Information provided by Polymer Te.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | |
LATI Latiblend 7587 E61-V0 PBT/PC, Flame Retardant Blend based on Polybutylene Terephthalate (PBT) / Polycarbonate (PC). Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability. High impact re.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | |
LATI Latimass 52/11-01 D020 PP Homopolymer Specific density compound based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.015 cm/cm @Thickness 3.20 mm |
0.011 - 0.015 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL GP3100 PP+MF10% Description: Injection Molding, PP+MF30%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |