Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | ASTM D955 |
PolyOne LubriOne™ NL-30GF/15T Black Polyamide 612 (Nylon 612) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 503 PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0040 cm/cm | 0.0010 - 0.0040 in/in | ASTM D955 |
PolyOne Dynaflex™ D3202-1000-03 Thermoplastic Elastomer (TPE) Dynaflex™ D3202-1000-03 is an easy processing TPE designed for general purpose applications and is suitable for injection molding, extrusion, blow molding, and thermoforming processes. - Dry Feel -.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | ASTM D955 |
PolyOne Edgetek® NY-20GF/10GB/000 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Lexan® ML3513 PC (Europe-Africa-Middle East) LEXAN ML3513 is a high viscosity, 30% short fibre glass reinforced, flame retardant grade, especially designed for connectors and relay separators.This data was supplied by SABIC-IP for the Europe-A.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Thickness 6.40 mm |
0.0020 - 0.0040 in/in @Thickness 0.252 in |
SABIC Method |
SABIC Innovative Plastics Lexan® FL930 PC Various weight reductions at 0.250"" (6.35 mm) wall, 30% GR. Superior flex strength/modulus, good tensile strength. V-0/5VA at 0.250"" (6.35 mm). |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0040 cm/cm | 0.0030 - 0.0040 in/in | ASTM D995 |
Kotec Carbotex KGN-20MRA Polycarbonate, Flame Retardant, 20% Glass Fiber Reinforced Features: Glass fiber 20% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E .. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0040 cm/cm | 0.0030 - 0.0040 in/in | |
LATI Later 4 G/50 PBT, 50% Glass Fiber Reinforced Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics ULTEM 2300R PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics ULTEM 2300R PEI (Europe-Africa-Middle East) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Ultem 2412EPR PEI (Europe-Africa-Middle East) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics ULTEM HU2310 PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Europe-Africa-Middle East) Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Stat-kon ZX05009 PPE+PS (Europe-Africa-Middle East) LNP* Stat-kon* ZX05009 is a compound based on PPE+PS Blend resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP EF006 PEI (Europe-Africa-Middle East) LNP* THERMOCOMP* EF006 is a compound based on Polyetherimide resin containing Glass Fiber. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® VB-8102G MPPE, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® F202G30 PBT, 30% Glass Filled, Fire Retardant, Halogen Free Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® P305G30 PP, 30% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | SABIC Method |
SABIC Innovative Plastics NORYL GFN2 PPE+HIPS (Asia Pacific) PPE+PS blend. 20% Glass reinforced. FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including pump.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0040 cm/cm | 0.0030 - 0.0040 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Lubricomp XL004 Amorphous Polyamide LNP* Lubricomp* XL-4040 is a compound based on Amorphous Nylon, containing PTFE.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0040 cm/cm | 0.0010 - 0.0040 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® EXVX1403 PBT (Asia Pacific) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | on Tensile Bar; E2P method |
Eurostar Starflam BFR460A PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR460A is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | ASTM D955 |
Clariant Renol PCSP0009 Polycarbonate, 15% Glass Fiber, Silicone Lubricated Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0040 cm/cm | 0.0030 - 0.0040 in/in | ASTM D955 |
Clariant Renol PP1100N40CC Polypropylene Homopolymer, 40% Glass Fiber and Mineral Reinforced, Chemically Coupled Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0040 cm/cm @Thickness 3.00 mm |
0.0030 - 0.0040 in/in @Thickness 0.118 in |
E2P method |
Eurostar Staramide PF003U PA6, 15% Glass Fiber Filled, Injection Molded Staramide PF003U is an 15% Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin, UV Stabilized (also known as Staramide 6 15V S4)Information provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | on Tensile Bar; E2P method |
Eurostar Staramide RF006XXP PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006XXP is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006)Information provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36HL PC LNP LUBRICOMP* DFL36HL is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable, Healthcare. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP JF006E PES (Europe-Africa-Middle East) LNP* Thermocomp* JF006E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding. |