Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.024 - 0.028 cm/cm
0.024 - 0.028 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP FL004 PE (Europe-Africa-Middle East)
LNP* Lubricomp* FL004 is a compound based on Polyethylene resin containing PTFE.
Linear Mold Shrinkage, Flow 0.024 cm/cm

@Time 86400 sec
0.024 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP FX04491H PE
LNP LUBRICOMP* FX04491H is a compound based on Polyethylene resin containing Proprietary Fillers. Added features of this material include: Wear Resistant.
Linear Mold Shrinkage, Flow 0.024 cm/cm

@Time 86400 sec
0.024 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP KI001XXJ Acetal
LNP* LUBRICOMP* KI001XXJ is a compound based on Acetal containing 2% Silicone. Added features of this grade include: Wear Resistant, Healthcare.
Linear Mold Shrinkage, Flow 0.024 - 0.027 cm/cm

@Thickness 3.20 mm
0.024 - 0.027 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® 337 PBT
Low temperature impact PBT. Automotive applications: underhood power distribution boxes and covers.
Linear Mold Shrinkage, Flow 0.024 cm/cm
0.024 in/in
SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific)
LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
Linear Mold Shrinkage, Flow 0.024 cm/cm

@Time 86400 sec
0.024 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific)
LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
Linear Mold Shrinkage, Flow 0.024 - 0.028 cm/cm
0.024 - 0.028 in/in
ISO DIS 294-4
Wellman Wellamid® XT1668-BK1 High Impact Nylon 66
Description: High Impact Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Flow 0.024 - 0.030 cm/cm

@Thickness 4.00 mm
0.024 - 0.030 in/in

@Thickness 0.157 in
E2P method
Eurostar Star L PA66 D61 PA66, Injection Molded
Star L PA66 D51 is a PTFE/Silicone Oil Lubricated, Unreinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Linear Mold Shrinkage, Flow 0.024 - 0.027 cm/cm

@Thickness 4.00 mm
0.024 - 0.027 in/in

@Thickness 0.157 in
E2P method
Eurostar Star L POM D84 POM, Injection Molded
Star L POM D84 is a PTFE/Proprietary Additive Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar.
Linear Mold Shrinkage, Flow 0.024 cm/cm
0.024 in/in
ISO 294-4
Barlog Plastics KEBAFLEX SG 50 A.1 black TPE-S, Shore A50, black
TPE-SInformation provided by BARLOG plastics GmbH.
Linear Mold Shrinkage, Flow 0.024 cm/cm
0.024 in/in
ISO 294-4
Barlog Plastics KEBAFLEX SG 65 A.01 TPE-S, Shore A65, natural
TPE-SInformation provided by BARLOG plastics GmbH.
Linear Mold Shrinkage, Flow 0.024 cm/cm
0.024 in/in
ISO 294-4
Barlog Plastics KEBAFLEX SG 60 A.01 black TPE-S, Shore A60, black
TPE-SInformation provided by BARLOG plastics GmbH.