Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.017 - 0.021 cm/cm | 0.017 - 0.021 in/in | ASTM D955 |
PolyOne Versaflex™ OM 6160-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 6160-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell.. |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm @Thickness 3.17 mm |
0.017 in/in @Thickness 0.125 in |
ASTM D955 |
Network Polymers Softflex® 0150 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.021 cm/cm | 0.017 - 0.021 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible B7500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.021 cm/cm | 0.017 - 0.021 in/in | ASTM D955 and ISO 294-4 |
Ravago Manufacturing Americas Hylon® N1000STHL HF Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer and LubricantFeatures: Lubricated, Heat Stabilized, High Flow and Ultra High ToughnessRoHS CompliantAuto Specifications: DELPHI DCM 4849 Color: B.. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.021 cm/cm @Thickness 3.17 mm |
0.017 - 0.021 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Hylon® N1000STHL UV2 Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Good Toughness, Lubricated, Heat StabilizedRoHS CompliantAuto Specifications: GM GMP.PA66.074 Color: BlackF.. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.020 cm/cm | 0.017 - 0.020 in/in | |
LATI Latan 13 S/30 POM, 30% Glass Bead Reinforced Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.018 cm/cm @Time 86400 sec |
0.017 - 0.018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing 10% PTFE, 15% Aramid. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.018 cm/cm @Time 86400 sec |
0.017 - 0.018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 (Asia Pacific) LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm @Thickness 3.17 mm |
0.017 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Electrablend® ABS 03106 MB Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm @Thickness 3.17 mm |
0.017 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 GB15 L BK 15% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 15% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Good UV Resistance and LubricatedAppearance: BlackTPCI# .. |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm @Thickness 3.17 mm |
0.017 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PP GB30 30% Glass Beads Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm @Thickness 3.17 mm |
0.017 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® PA6 TL10 Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (10%)Features: Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm @Thickness 3.17 mm |
0.017 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® PA6 TL15 Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (15%)Features: Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.026 cm/cm @Thickness 3.20 mm |
0.017 - 0.026 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® K3501 PBT Unfilled PBT, Hydrollytically Stable, Heat Stabilized, Impact Modified. A hydrollytically stable grade designed for improved performance under heat/humidity environments. Targeted at automotive unde.. |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | 24 hours + 30 min at 93°C |
Teknor Apex TEKRON® 4300LM-P86-1 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | Sim. To ISO 294-4 |
DSM Arnite® BM4 240 (PBT+PET)-MD20 20% Mineral Reinforced |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® S610SF BK851 Polybutylene Terephthalate (PBT) Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin S610SF is an unreinforced low viscosity polybutylene terephthalate for injection molding. It has hig.. |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm @Thickness 4.00 mm |
0.017 in/in @Thickness 0.157 in |
E2P method |
Eurostar Staramide P1000J5 PA6, Impact Modified, Injection Molded Staramide P1000J5 is a Low Temperature Impact Modified, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | Eurotec |
Eurotec® Tecodur® PB70 BK001 HS PBT, unfilled, improved impact, heat stabilized, black Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | ASTM D955 |
Clariant Renol 6253-L UV Nylon 6, High Impact, Lubricated, UV Stabilized Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me.. |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Hytrel® HTR8685 BK022A Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Hytrel HTR8685 BK022A is designed for blow molding or processing techniques requi.. |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | ASTM D955 |
Clariant Renol PA111BK S&P Nylon 66, General Purpose Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | Eurotec |
Eurotec® Tecomid® NA40 NL IH PA6.6, impact modified, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm @Thickness 2.00 mm |
0.017 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit.. |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | Sheet |
BASF Ultradur® B 4300 M2 12.5% Mineral Filled PBT Description: Is a PBT-HI, mineral-reinforced, impact-modified injection-molding grade for rigid parts, for example automotive power door locks.Information provided by BASF |
|||
Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | ISO 294-4 |
DuPont Performance Polymers Crastin® S610SF NC010 PBT
(Unverified Data**) Crastin® S610SF is an unreinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast production.Informati.. |