Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0023 cm/cm | 0.0023 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP BG004 SAN (Europe-Africa-Middle East) LNP* LUBRICOMP* BG004 is a compound based on Styrene Acrylonitril resin containing Graphite. Added features include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.0023 cm/cm | 0.0023 in/in | ISO 294-4, 2577 |
Lanxess Durethan® BKV 30 EF 000000 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, low viscosity (Easy Flow) |
|||
Linear Mold Shrinkage, Flow | 0.0023 cm/cm | 0.0023 in/in | ISO 294-4, 2577 |
Lanxess Durethan® DP 1852/30 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glassfibers, UL V-0 at 0.75 mm (listed),GWIT:775°C at 0,75 mm, GWFI:960°C at 0.75 mm, CTI/A:400, good flowabilityApplication Examples: Hand-held barrel pump housings |
|||
Linear Mold Shrinkage, Flow | 0.0023 cm/cm | 0.0023 in/in | ISO 294-4, 2577 |
Lanxess Pocan® DP 2004 000000 PBT PBT, non-reinforced, injection molding, halogen free flame retardant |
|||
Linear Mold Shrinkage, Flow | 0.0023 cm/cm | 0.0023 in/in | 60x60x2; 280°C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Durethan® BKV 30 H2.0 EF DUS029 901510 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.0023 cm/cm | 0.0023 in/in | 60x60x2; 280°C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Durethan® BKV 35 H3.0 000000 Nylon 6, Glass Fiber Reinforced PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.0023 cm/cm | 0.0023 in/in | |
Solvay TECHNYLSTARâ„¢ SX 216 V50 PA6, 50% glass filled, DRY Description: TECHNYLSTAR Polyamide, reinforced with 50% of glass fiber, characterized by a high fluidity of the melt, for injection molding.Available in: Asia Pacific, Europe and North America Produ.. |
|||
Linear Mold Shrinkage, Flow | 0.0023 cm/cm | 0.0023 in/in | SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP ZF006 PPE+PS (Europe-Africa-Middle East) LNP* THERMOCOMP* ZF006 is a compound based on PPE+PS Blend resin containing Glass Fiber |
|||
Linear Mold Shrinkage, Flow | 0.0023 - 0.0028 cm/cm @Thickness 3.20 mm |
0.0023 - 0.0028 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX8721 PPE+PA Noryl GTX GTX8721 resin is a glass and talc filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, conductivity, and low warpage. This .. |
|||
Linear Mold Shrinkage, Flow | 0.0023 - 0.0043 cm/cm @Time 86400 sec |
0.0023 - 0.0043 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Verton RV008ESV_GY7E072 PA 66 Preliminary data for 40% long glass fiber filled, single color pellet gray, PA66This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.0023 cm/cm @Thickness 2.00 mm |
0.0023 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66
(Unverified Data**) Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.0023 cm/cm @Time 86400 sec |
0.0023 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON RX970079 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RX970079 is a compound based on PA 66 resin containing Long Glass Fiber and PTFE. Added features include; Internally Lubricated. |