Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0010 - 0.0040 cm/cm | 0.0010 - 0.0040 in/in | ASTM D955 |
Polymer Resources PC-G20-[color]-1 Polycarbonate, 20% Glass Reinforced with Mold Release Polycarbonate, 20% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | (longitudinal) Injection and Compression; ISO 2577 |
Raschig Group EPOXIDUR® 3580 EP Epoxy Glass-fiber reinforced and mineral filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties even with thin wall thicknesses and high temperatures. This prod.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0040 cm/cm | 0.0010 - 0.0040 in/in | |
Lehmann & Voss LUVOCOM® 1105-8205 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0040 cm/cm | 0.0010 - 0.0040 in/in | |
Lehmann & Voss LUVOCOM® 1105-0699-1 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | |
Lehmann & Voss LUVOCOM® 50/GF/20/TF/20/GY Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | ASTM D955 |
Sumitomo Bakelite North America E 2748-9641D Short Glass Fiber Reinforced Epoxy E 2748-9641D is a mineral and short fiberglass filled epoxy molding compound.Information provided by Sumitomo Bak North America, Inc. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0040 cm/cm | 0.0010 - 0.0040 in/in | ASTM D955 |
PlastxWorld CEVIAN® VGR30 30% GF ABS Glass fiber reinforced ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0040 cm/cm | 0.0010 - 0.0040 in/in | typical. |
Cosmic Plastics CP7311 Epoxy Molding Compound Data provided by the manufacturer. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0040 cm/cm | 0.0030 - 0.0040 in/in | |
Polyram PlusTek PA301G6 Nylon 6.6, Heat Stabilized, 30% Glass Fiber Heat stabilized, 30% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0040 cm/cm | 0.0010 - 0.0040 in/in | typical. |
Cosmic Plastics D72 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0040 cm/cm | 0.0010 - 0.0040 in/in | typical. |
Cosmic Plastics E4930 Mineral & Glass Filled Epoxy Molding Compound, Encapsulated Grade Data provided by the manufacturer. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | |
Polyram RamOfin PPH300J8 Polypropylene, 40% Glass Fiber 40% glass fiber and glass beads reinforced, high stiffness polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | ASTM D955 |
Diamond Polymers ABS 3501 GF-10 Description: Reinforced Grade, 10%Glass FilledInformation provided by Diamond Polymers, Inc. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0040 cm/cm | 0.0030 - 0.0040 in/in | |
BCC Products BC 9020 Silicone RTV Rubber BC 9020 is a violet colored, two-component, flowable compound that regardless of thickness or confinement, cures at room temperature. The cured rubber is high strength and high tear with good elonga.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0040 cm/cm | 0.0010 - 0.0040 in/in | ASTM D955 |
Cheng Yu Plastic A702G1 ABS 10% Glass Fiber Reinforced |
|||
Linear Mold Shrinkage | 0.0030 - 0.0040 cm/cm | 0.0030 - 0.0040 in/in | ASTM D955 |
PolyOne Edgetek® PI-20GF/000 Polyetherimide (PEI), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | ASTM D-955 |
Axiall 5009 Rigid PVC, Molding Georgia Gulf 5009 is a type I, Grade I rigid vinyl injection molding compound designed for fittings and parts of similar confiation where maximum tensile strength and/or chemical resistance is requi.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0040 cm/cm | 0.0030 - 0.0040 in/in | ASTM D955 |
PolyOne Edgetek® PI-10CF/000 Polyetherimide (PEI), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedElectrically ConductiveInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0040 cm/cm | 0.0030 - 0.0040 in/in | ASTM D955 |
PolyOne Edgetek® AM-30GF/000 Polyphthalamide (PPA), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | ISO 2577 |
Polyram PlusTek RA320G5 Nylon 66 for Injection Molding, 25% Glass-Fiber Reinforced, Flame Retardant and High Stiffness 25% Glass-fiber reinforced, flame retardant and high stiffness Nylon 66 for injection molding applications.Information provided by Polyram. |