Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | |
Nylene® Naxel™ PC10 Polycarbonate Description: Naxel™ PC10 is a 9 melt, general purpose polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources C.. |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | |
Nylene® Naxel™ PC1210 Polycarbonate Description: Naxel™ PC1210 is a 6 melt, general purpose polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm | 0.0060 - 0.010 in/in | ASTM D955 |
Network Polymers PC-1029 AS/P Description: Antistatic PolycarbonateInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYabs N30 ABS Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | ASTM D955 |
Polymer Resources PC-HH Polycarbonate, High Heat Polycarbonate, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resource.. |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | LATI |
LATI LATILUB 88/50-20GRT K/10 PEEK Based, 10% Carbon Fiber Reinforced, 20% Graphite and PTFE Self Lubricating Plastic Latilub self-lubricating plastic materials are designed to replace metals in applications such as gears, bushings, cams, slides, etc., for which, besides their intrinsic properties (moldability, low.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYabs F00L ABS Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0060 - 0.013 cm/cm | 0.0060 - 0.013 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 HH-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | Compression; ASTM D955 |
Plaslok 202 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 202 is a two-stage, woodflour-filled .. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | |
Lehmann & Voss LUVOCOM® 50/TF/15/BK-1 Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.014 cm/cm | 0.0060 - 0.014 in/in | ASTM D955 |
Kolon SPESIN® KP212G15V0BM G/F Reinforced & Flame Retardant PBT Compound Resin Flame retardant, paintabilityApplications: A variety of cases and connectorsInformation provided by API-Kolon. |
|||
Linear Mold Shrinkage | 0.0060 - 0.013 cm/cm | 0.0060 - 0.013 in/in | |
Lehmann & Voss LUVOCOM® 1-7032-B Polyamide 66, with aramid reinforcement and PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved wear behaviour, low warpage.Improved heat resistance.Control disks, cams, sliding elem.. |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | |
Styron CALIBRE™ 300EP 22 Polycarbonate, General Purpose CALIBRE® 300EP series resins are general purpose polycarbonate resins and can be supplied with a mold release package, a UV stabilizer package or both. CALIBRE 300EP resins exhibit an excellent p.. |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | ASTM D955 |
Tipco Tipcolite® TX 311 Phenolic Compound, Wood Flour & Minerals, having Soft Flow & High Strength Soft Flow Phenolic Compound, Reinforced with Wood Flour & MineralsApplications: Switchgear, HRC FusesProcessing: Injection MouldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
I.. |
|||
Linear Mold Shrinkage | 0.0060 cm/cm @Thickness 2.00 mm |
0.0060 in/in @Thickness 0.0787 in |
|
Toyobo PELPRENE™ P80C Polyester TPE, High Flexibility, High Melting Point Features: Polyester TPE, High Flexibility, High Melting PointInformation provided by Toyobo. |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | GB/15585 |
Zhejiang Juner PC-A2 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | ASTM D955 |
Eastman Tritan TX1800 Copolyester Applications:Consumer and durable goodsExtrusion blow moldingInjection stretch blow moldingKey Attributes:Ease of processingExcellent clarityExcellent Hydrolytic stabilityGood chemical resistanceGoo.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | ASTM D 955 |
Cossa Polimeri ESTAPROP H 0560 GFCTG Polypropylene, 30% Mixed Filler PP homopolymer 30% mixed fillerGood physical and mechanical characteristicsInformation provided by Cossa Polimeri S.r.l. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm | 0.0060 - 0.010 in/in | ASTM D955 |
Diamond Polymers ASA TWP 121 Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc. |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | |
E-Polymers TEKANATE® G7013 General Purpose Easy Molding Polycarbonate Modified Poly Carbonate: TEKANATE is a modified PC by improving polycarbonate resins with features of halogen-free flammability, transparency, impact resistance and reinforced fiberglass. It shows .. |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | MD; ASTM D955 |
Aclo Accucomp ABS ABS811L Medium Impact Grade |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | Compression; ASTM D955 |
Chang Chun Plastic Longlite PM T310 Impact Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | ASTM D955 |
Ashley Polymers Ashlene® 1041BU Polycarbonate A general purpose injection molding grade, in black. Also available as: 1043BU (with UV stabilizers).Data provided by the manufacturer |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | ASTM D955 |
Aaron Industries AAROLENE® ARPS HI-100-4 Polystyrene Compounded Resin AAROLENE® ARPS 100 Series Polystyrene Compounded ResinColor may be specified. Melt Flow Index may be specified. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm |
0.0060 - 0.010 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 392 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | ASTM D955 |
PlastxWorld CEVIAN® B45M0 PBT/ABS Alloy These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |