Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00080 cm/cm | 0.00080 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 1268 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1268 is a fiberglass reinforced thermoset thick molding compound for composite power train applications such as valve covers and timing gear covers.Key features and benefits are:Ideal f.. |
|||
Linear Mold Shrinkage | 0.00080 - 0.0060 cm/cm @Thickness 4.00 mm, Temperature 23.0 °C |
0.00080 - 0.0060 in/in @Thickness 0.157 in, Temperature 73.4 °F |
Flow Bergmann Method; ISO 294-4 |
PolyOne Bergamid™ B70 G45 BK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Linear Mold Shrinkage | 0.00080 cm/cm | 0.00080 in/in | ATM D955 |
Plenco 50045 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 50045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is UL listed and available in white, natural, and black.Information s.. |
|||
Linear Mold Shrinkage | 0.00080 cm/cm | 0.00080 in/in | ASTM D955 |
North Wood Plastics PS with 40% Wood Fiber Data provided by North Wood Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.00080 cm/cm | 0.00080 in/in | ISO 2577 |
Menzolit Menzolit® BMC 1650 Unsaturated Polyester UP BMC 1650 is a specially designed anti-microbial polyester moulding compound which incorporates a "germ killer" . It has been tested and found to be compliant for resistance to fungal defacement in .. |
|||
Linear Mold Shrinkage | 0.00080 cm/cm | 0.00080 in/in | ISO 2577 |
Menzolit Menzolit® SMC 0600 Unsaturated Polyester UP SMC 0600 is a specially formulated SMC for reduced moulding pressure (< 30 bar). The glass level has been selected to combine good mouldability with strength and stiffness. Even without a specific f.. |
|||
Linear Mold Shrinkage | 0.00080 cm/cm | 0.00080 in/in | ISO 2577 |
Menzolit Menzolit® SMC 0900 Unsaturated Polyester UP SMC 0900 is a special SMC for use within a chemical aggressive environment. The glass level is selected to combine good mouldability with good strength and stiffness properties. The product is espec.. |
|||
Linear Mold Shrinkage | 0.00080 cm/cm | 0.00080 in/in | ISO 2577 |
Menzolit Menzolit® SMC 1000 Unsaturated Polyester UP SMC 1000 is a special SMC for hydrolysis resistant applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Typical applications are .. |
|||
Linear Mold Shrinkage | 0.00080 cm/cm | 0.00080 in/in | ISO 2577 |
Menzolit Menzolit® SMC 2300 Unsaturated Polyester UP SMC 2300 is an arc resistance SMC for arc quenching cambers. High fire retardancy SMC for electrical applications .Information Provided by Menzolit |
|||
Linear Mold Shrinkage | 0.00080 cm/cm | 0.00080 in/in | ISO 2577 |
Menzolit Menzolit® BMC 0300 Unsaturated Polyester UP BMC 0300 is a low shrink standard material for general-purpose applications, which require a higher level on surface quality and better dimensional stability. The glass content is on a level that co.. |
|||
Linear Mold Shrinkage | 0.00080 cm/cm | 0.00080 in/in | ISO 2577 |
Menzolit Menzolit® BMC 2300 Unsaturated Polyester UP BMC 2300 is a special BMC with exceptional high fire retardancy. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. Fire retardanc.. |
|||
Linear Mold Shrinkage | 0.00080 cm/cm | 0.00080 in/in | ISO 2577 |
Menzolit Menzolit® SMC 0300 Unsaturated Polyester UP SMC 0300 is a low shrink standard SMC providing improved surface quality, reduced shrinkage and warpage. Typical fields of applications are mechanical engineering and electrical industry, where impr.. |
|||
Linear Mold Shrinkage | 0.00080 cm/cm | 0.00080 in/in | ISO 2577 |
Menzolit Menzolit® SMC 2400 Unsaturated Polyester UP SMC 2400 is a SMC with fire retardancy. The glass level has been selected to combine mouldability with strength and stiffness properties. The fire retardancy is especially high, and the material is .. |
|||
Linear Mold Shrinkage | 0.00080 cm/cm | 0.00080 in/in | average process; cross flow; 150x80x2mm |
Borealis Xmod™ GD302HP Polypropylene, Glass Fiber Reinforced Xmod™ GD302HP is a 30 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. This material has an excellent balance between impact stre.. |
|||
Linear Mold Shrinkage | 0.00080 cm/cm | 0.00080 in/in | Bayer Test |
Covestro Bayfill® EA 2002 Polyurethane Energy-Absorbing Semi-Rigid Foam, Friable Grade, MDI-based 2-Component Liquid System Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Linear Mold Shrinkage | 0.00080 cm/cm | 0.00080 in/in | ASTM D2566-69 |
BCC Products Kwik Kast BC 8645 Urethane Casting BCC Kwik Kast/Gray is a two component, fast setting polyurethane reproduction plastic. BC8645 has been reformulated to enhance filler suspension and avoid hard packing @ 77ºF. Uses include; tracing.. |
|||
Linear Mold Shrinkage | 0.00080 cm/cm | 0.00080 in/in | |
BCC Products METAL-KAST/SLO BC 8010-2 Urethane Casting BC8010-2 Metal-Kast/Slo, the result of extensive research and development is an aluminum filled, metal-like, medium setting urethane reproduction plastic. A slower version of the BC8010 Metal-Kast w.. |
|||
Linear Mold Shrinkage | 0.00080 cm/cm | 0.00080 in/in | ASTM D955 |
Bulk Molding Compounds BMC 940 Vinyl Ester Bipolar Plate Material Product Introduction: Bulk Molding Compounds, Inc. is the largest manufacturer of thermoset bulk molding compounds in North America, serving the automotive, appliance, and electrical markets. BMC t.. |
|||
Linear Mold Shrinkage | 0.00080 cm/cm | 0.00080 in/in | |
BCC Products Kwik Kast BC 8001 Urethane Casting BC8001 is an advanced fast cast polyurethane tooling system. It features low viscosity, low exotherm and minimal shrinkage. It cures hard, yet more durable resulting in less brittle parts. Designed.. |
|||
Linear Mold Shrinkage | 0.00080 cm/cm | 0.00080 in/in | |
BCC Products Kwik Kast BC 8002 Urethane Casting Kwik Kast II is an enhanced fast cast polyurethane tooling system. It has been reinvented for greater moisture resistance and improved filler suspension for easier premixing of the components. Kwik.. |
|||
Linear Mold Shrinkage | 0.00080 cm/cm | 0.00080 in/in | |
BCC Products Kwik Kast BC 8650 Urethane Casting BC 8650 is an advanced fast cast polyurethane tooling system. BC 8650 features low viscosity, low exotherm and minimal shrinkage. Kwik Kast Blue cures hard, yet more durable resulting in less brittl.. |