Physical Properties Metric English Comments
Linear Mold Shrinkage 0.013 - 0.015 cm/cm
0.013 - 0.015 in/in
With Flow; ISO 2577
Polykemi AB POLYelast TPE R44 Thermoplastic Elastomer
Information provided by Polykemi AB
Linear Mold Shrinkage 0.0050 - 0.015 cm/cm
0.0050 - 0.015 in/in
FRISETTA Test Method
Nilit FRIANYL A63 FK 1020 Nylon 6.6 for injection molding, 10% glass fiber and 20% glass ball reinforced
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
Linear Mold Shrinkage 0.011 - 0.015 cm/cm
0.011 - 0.015 in/in
ASTM D955
Polymer Resources NY6-GP1 General Purpose Nylon 6
General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry ..
Linear Mold Shrinkage 0.011 - 0.015 cm/cm
0.011 - 0.015 in/in
ASTM D955
Polymer Resources NY6-GP1-[color]H Nylon, General Purpose, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Linear Mold Shrinkage 0.010 - 0.015 cm/cm
0.010 - 0.015 in/in
FRISETTA Test Method
Nilit FRIANYL A63 CV40 Nylon 6.6 for injection molding, 40% carbon fiber reinforced
Nylon 6.6 for injection molding (good conductive and electrostatic properties).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Linear Mold Shrinkage 0.0080 - 0.015 cm/cm
0.0080 - 0.015 in/in
FRISETTA Test Method
Nilit FRIANYL A63 HS-GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced
Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Linear Mold Shrinkage 0.0050 - 0.015 cm/cm
0.0050 - 0.015 in/in
FRISETTA Test Method
Nilit FRIANYL B63 MG30 Nylon 6 for injection molding, 30% mineral filled
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Linear Mold Shrinkage 0.0090 - 0.015 cm/cm
0.0090 - 0.015 in/in
Lehmann & Voss LUVOCOM® 1105-8127 PEEK, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
Linear Mold Shrinkage 0.011 - 0.015 cm/cm
0.011 - 0.015 in/in
Lehmann & Voss LUVOCOM® 3-8266 Polyamide 6, unreinforced
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
Linear Mold Shrinkage 0.010 - 0.015 cm/cm
0.010 - 0.015 in/in
Lehmann & Voss LUVOCOM® 6-8503/BL Polyamide 12, unreinforced
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion.Isotropic shrinkage characteristics.Bearings, sleeve..
Linear Mold Shrinkage 0.013 - 0.015 cm/cm
0.013 - 0.015 in/in
ASTM D955
Kolon KOPA® KN131 General Purpose Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Linear Mold Shrinkage 0.013 - 0.015 cm/cm
0.013 - 0.015 in/in
ASTM D955
Kolon KOPA® KN136 General Purpose Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Linear Mold Shrinkage 0.0080 - 0.015 cm/cm
0.0080 - 0.015 in/in
ASTM D955
Samyang Tramid® 210F Polyamide, High Productivity
Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210F is a high productivity grade.Applications:ConnectorsCable tiesHarness clipsT..
Linear Mold Shrinkage 0.012 - 0.015 cm/cm
0.012 - 0.015 in/in
ASTM D955
Samyang Tramid® 215 Polyamide, High Impact
Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.215 is a high impact grade.Applications:Automotive knob types, door handles and m..
Linear Mold Shrinkage 0.014 - 0.015 cm/cm
0.014 - 0.015 in/in
ASTM D955
Samyang Triel® 5400 Thermoplastic Polyether Ester Elastomer
TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r..
Linear Mold Shrinkage 0.011 - 0.015 cm/cm
0.011 - 0.015 in/in
ISO 2577
Polyram RamOfin PPH343T4BK10 Polypropylene, 20% Mineral Filled
20% Mineral filled, heat resistant polypropylene for injection molding applications.Information provided by Polyram.
Linear Mold Shrinkage 0.011 - 0.015 cm/cm

@Thickness 3.20 mm
0.011 - 0.015 in/in

@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 391 Ionomer
DescriptionFormion® FI 391 is a non-reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low temperature ductility, and medium stiffness. Formion F1 391U i..
Linear Mold Shrinkage 0.011 - 0.015 cm/cm

@Thickness 3.20 mm
0.011 - 0.015 in/in

@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 391 Ionomer
DescriptionFormion® FI 391 is a non-reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low temperature ductility, and medium stiffness. Formion F1 391U i..
Linear Mold Shrinkage 0.0080 - 0.015 cm/cm
0.0080 - 0.015 in/in
ASTM D955
Cheng Yu Plastic N6C2 Nylon 6, 20% Mineral Reinforced
Linear Mold Shrinkage 0.0080 - 0.015 cm/cm
0.0080 - 0.015 in/in
ASTM D955
Cheng Yu Plastic N6CV3 Flame Retardant Nylon 6, 30% Mineral Reinforced
Linear Mold Shrinkage 0.0080 - 0.015 cm/cm
0.0080 - 0.015 in/in
ASTM D955
Cheng Yu Plastic N6GV15 Flame Retardant Nylon 6, 15% Glass Filled
Linear Mold Shrinkage 0.0080 - 0.015 cm/cm
0.0080 - 0.015 in/in
ASTM D955
Cheng Yu Plastic N6GV20 Flame Retardant Nylon 6, 20% Glass Filled
Linear Mold Shrinkage 0.0025 - 0.015 cm/cm
0.0025 - 0.015 in/in
ASTM D955
EPICHEM Epiter PBT GF 30 Polybutylene Terephthalate, 30% Glass
Characteristics: 30% glass fibre filled
Linear Mold Shrinkage 0.010 - 0.015 cm/cm
0.010 - 0.015 in/in
ASTM D955
Beijing Chemical Industry KAIFA® 201-G15R PBT Resin
20% glass fiber reinforced, good flow and toughnessInformation provided by Beijing Chemical Industry Research Institute (Group)
Linear Mold Shrinkage 0.0050 - 0.015 cm/cm
0.0050 - 0.015 in/in
ASTM D955
Cheng Yu Plastic FV30G15 POM, 15% Glass Fiber