Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | |
Polycasa XT 620 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | |
Polycasa XT 630 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0090 cm/cm | 0.0050 - 0.0090 in/in | (longitudinal) Compression; ISO 2577 |
Raschig Group MELOPLAS® 181.5 MF Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. Very good electrical properties, high surface hardness, good mechanical strength, high UV and heat resis.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | ASTM D955 |
Polymer Resources TP-G30 Polybutylene Terephthalate, 30% Glass Reinforced Polybutylene Terephthalate, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Linear Mold Shrinkage | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ASTM D955 |
Multibase Multi-Pro® 5002 CU Natural Polypropylene Forms:PelletsProcessing Methods:Injection MoldingFeatures:Gloss, LowInformation provided by Multibase |
|||
Linear Mold Shrinkage | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ASTM D955 |
PolyOne Edgetek® PI-1000 Polyetherimide (PEI)
(discontinued **) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Linear Mold Shrinkage | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ASTM D955 |
LyondellBasell SEQUEL® E3000 TPO Description: SEQUEL® E3000 thermoplastic olefinic elastomer (TPO) is designed for thermoformed exterior and interior applications that require toughness and dimensional stability. This extrusion.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | |
Lehmann & Voss LUVOCOM® 80-7555 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | |
Lehmann & Voss LUVOCOM® 80-7555/BK Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0090 cm/cm @Temperature 23.0 °C |
0.0060 - 0.0090 in/in @Temperature 73.4 °F |
Plumb; ASTM D955 |
Kingfa JE2-R2G20 Glass Fiber Reinforced ABS/PBT Alloy Features:High stiffness, high hardnessGood mechanical strengthGood chemical resistanceGood size stabilityGood heat stabilityLow tendency to warpApplications:Optical appliance (camera, video)Sports a.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0090 cm/cm @Temperature 23.0 °C |
0.0030 - 0.0090 in/in @Temperature 73.4 °F |
ASTM D955 |
Kingfa PBT-RG301 Flame Retardant, 30% Glass Fiber Reinforced PBT Features:Flame retardantHigh mechanical strengthHigh heat resistanceGood electric propertiesNo bloomingApplications:Injection moldingHousehold appliance partsBobbinLighting partsRelayLinkerInformati.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0090 cm/cm @Temperature 23.0 °C |
0.0040 - 0.0090 in/in @Temperature 73.4 °F |
ASTM D955 |
Kingfa PA66-G30 30% Glass Fiber Reinforced PA66 Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0090 cm/cm | 0.0050 - 0.0090 in/in | ISO 294-4 |
Styrolution Luran® S 767KE ASA Luran S 767KE is particular suitable for co-extrusion with PVC at low temperature. Hereby, it provides a glossy surface finish.Enhanced flowabilitySuitable for co-extrusion with PVCEnables high glos.. |
|||
Linear Mold Shrinkage | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ASTM D955 |
PlastxWorld CEVIAN® B1500 PBT/ABS Alloy Unfilled, Excellent ToughnessThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0090 cm/cm | 0.0050 - 0.0090 in/in | ISO 294-4 |
Wellman Wellamid® GF13-66 XE-N 13% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0090 cm/cm | 0.0050 - 0.0090 in/in | D955 |
Zhejiang Juner 301-G15 15% Glass Fibre Reinforced and Flammable Resistant Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0090 cm/cm @Thickness 3.20 mm, Time 259000 sec |
0.0050 - 0.0090 in/in @Thickness 0.126 in, Time 72.0 hour |
ISO 294 |
A. Schulman FORMION™ FI 233 15% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 233 is an injection molding grade, 15% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. A.. |
|||
Linear Mold Shrinkage | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | |
Ecomass® 1850ZC84 Stainless Steel Powder Filled Polyamide (PA6), Injection Molding Stainless Steel Powder Filled Polyamide (PA6), Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and radiation shielding a.. |
|||
Linear Mold Shrinkage | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ASTM D955 |
Diamond Polymers DIAMALOY 310 GF10 PC/Polyester Alloy, Impact Modified Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | ASTM D955 |
Diamond Polymers DIAMALOY 530 PC/PBT Alloy, UV Stabilized/Weatherable Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Linear Mold Shrinkage | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | |
E-Polymers TEKAMID® JN110 PPE+PA66 Filler Reinforced PA/PPE Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0090 cm/cm | 0.0040 - 0.0090 in/in | ASTM D955 |
Asia International Enterprise (Hong Kong) 60G7F Nylon 66, 35% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |