Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00200 - 0.00500 cm/cm | 0.00200 - 0.00500 in/in | Average value: 0.00350 cm/cm Grade Count:8 |
Overview of materials for PVC, High Impact This property data is a summary of similar materials in the MatWeb database for the category "PVC, High Impact". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00500 cm/cm | 0.00100 - 0.00500 in/in | Average value: 0.00325 cm/cm Grade Count:12 |
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 20% Glass Fiber". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00500 cm/cm | 0.00100 - 0.00500 in/in | Average value: 0.00269 cm/cm Grade Count:8 |
Overview of materials for Glass Reinforced, Modified SMA This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00500 cm/cm | 0.00100 - 0.00500 in/in | Average value: 0.00288 cm/cm Grade Count:3 |
Overview of materials for Nylon 11 with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are includ.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron HR60N ABS Heat Resistant High ImpactInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron IPM3000 PMMA- ABS Alloy Super High Gloss, High scratch resistanceInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU602 ABS Heat Resistant High ImpactInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU650N ABS Heat Resistant Medium/High ImpactInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron TG3MM ABS Injection Molding Grade Medium Flow, Medium Impact, high RigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS 2000 Glitter SAN Resin High Transparent SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU650N ABS Heat Resistant Medium/High ImpactInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron TG3MM ABS Injection Molding Grade Medium Flow, Medium Impact, high RigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS1000 Sparkle SAN Resin High Transparent SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU660 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU670 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU670M ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS 2000 SAN Resin Clear SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS 2007LF SAN Resin High Rigidity Clear SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron IM14GM ABS Injection Molding Grade High Rigidity, Medium Impact, Good paintabilityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU650NH ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU670M ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS 2000 Glitter SAN Resin High Transparent SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS 2006 SAN Resin Very High Rigidity Clear SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS1000 SAN Resin Clear SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS1000M SAN Resin Clear SAN, Pen barrel applicationInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00100 - 0.00500 cm/cm | 0.00100 - 0.00500 in/in | Average value: 0.00232 cm/cm Grade Count:21 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU602M ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00100 - 0.00500 cm/cm | 0.00100 - 0.00500 in/in | Average value: 0.00356 cm/cm Grade Count:16 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and .. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS1000 Sparkle SAN Resin High Transparent SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron IM14GL ABS Injection Molding Grade Super High Rigidity, Medium Impact, High Chemical ResistanceInformation provided by Bhansali |