Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Network Polymers Kepital® F10-02 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Oxford Polymers C-Acetal 25GF 25% Glass Fiber Reinforced Copolymer Acetal 25% Glass Fiber Reinforced Copolymer AcetalInformation provided by Oxford Polymers. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | STN 64 0808 |
Plastcom SLOVALEN PC 53 N Polypropylene Copolymer, UV Stabilization FeaturesModified copolymer PP for injection moulding, with the ability of modeling the melt flow rate within the interval 5 - 20 g/10 min. Can be used for simple small as well as for large complica.. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Global POM-270 Low Melt Acetal Information provided by Global Polymers Corporation. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Global POM-90 General Purpose Acetal Information provided by Global Polymers Corporation. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | |
Shin-Etsu Silicones LIMSâ„¢ KE2004-20A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | |
Shin-Etsu Silicones LIMSâ„¢ KE1950-35A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Aclo Accucomp Polyacetal (POM) ACE091L High Viscosity |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Aaron Industries AAROLENE® ARPP 200-2 PP Black Polypropylene Copolymer AAROLENE® ARPP 200 Series Polypropylene Compounded ResinFeatures: A high flow polypropylene copolymer resin, pre-colored black, specifically designed for all high speed injection molding applicati.. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Aaron Industries AVPP C 200-2 Virgin Polypropylene Melt flow index may be specified. |
|||
Linear Mold Shrinkage | 0.022 cm/cm @Thickness 4.00 mm |
0.022 in/in @Thickness 0.157 in |
|
Azoty Tarnow™ TARNOFORM 300 CI4 POM Impact modified injection molding grade based on Tarnoform 300 reinforced with 20% MBS rubber yielding good cold impact strength and good strength of weld lines combined with good weatherability.Inf.. |
|||
Linear Mold Shrinkage | 0.022 cm/cm @Thickness 2.00 mm |
0.022 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, Conditioned Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To.. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Ashley Polymers Ashlene® 192-N2 Acetal A general purpose, high viscosity, natural.Data provided by the manufacturer |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Ashley Polymers Ashlene® 195-N2 Acetal A general purpose, medium viscosity natural.Data provided by the manufacturer |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Ashley Polymers Ashlene® 197-N2 Acetal A general purpose, very low viscosity, in natural.Data provided by the manufacturer |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Oxford Polymers H-Acetal 20PTFE 20% PTFE Reinforced Homopolymer Acetal
(discontinued **) 20% PTFE Reinforced Homopolymer AcetalInformation provided by Oxford Polymers. |
|||
Linear Mold Shrinkage | 0.022 cm/cm @Thickness 2.00 mm |
0.022 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 67B Nylon 66, General Purpose, very high viscosity, Conditioned Vydyne® 67B is a very-high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67B resin offers high strength, rigidity and.. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Mitsubishi Iupital® F10-02 High Viscosity Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Linear Mold Shrinkage | 0.022 - 0.024 cm/cm | 0.022 - 0.024 in/in | ASTM D955 |
PolyOne Lubri-Tech™ 5209 S2 Natural A Acetal Copolymer, 9 Melt with Silicone
(discontinued **) Information provided by PolyOne™ Corporation |