Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | ASTM D955 |
Multibase Multi-Pro® 3014 CUW Polypropylene Calcium Carbonate Filler, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | ASTM D955 |
RheTech Products FT3080-729UV Thermoplastic Polyolefin, UV Stabilized, AG-64 Grey Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | ASTM D955 |
RheTech Products FT3080-81 Thermoplastic Polyolefin, UV Stabilized, ACRA Titanium Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPC T12020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPC TS15020E Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPC TS20020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPH T4020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | Across Flow; ISO 2577 |
Polykemi AB SCANMID 6 B12^ NH9 Nylon 6, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPH T3022D Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | per ATM D955. Post shrinkage is 0.29% at 72hr 120ºC per ASTM D1299. |
Plenco 2424 Phenolic, Granular, Injection Molded
(discontinued **) Two-stage Phenolic. PLENCO 02424 is a black, two stage, general purpose phenolic molding compound. It has a good balance of properties for a general purpose type material. It is used in electrical .. |
|||
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | |
Lehmann & Voss LUVOCOM® 1105-7194/GY PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Linear Mold Shrinkage | 0.010 - 0.018 cm/cm | 0.010 - 0.018 in/in | |
Lehmann & Voss LUVOCOM® 19-7810 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | ASTM D955 |
Sumitomo Bakelite Durez® 152 Phenolic, Compression Grade Durez 152 Phenolic is a two-stage, heat resistant/electrical molding material. It exhibits superior dimensional stability, good strength retention at elevated temperature and good molded appearance.. |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | Isotropy |
Solvay TECHNYL® A 205F PA66, DRY Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Linear Mold Shrinkage | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | |
Borealis BE375MO Polypropylene Copolymer BE375MO is a heterophasic copolymer. This grade is characterized by optimum combination of high impact strength and stiffness. This grade is formulated for an excellent antistatic performance. Elect.. |
|||
Linear Mold Shrinkage | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | |
Borealis BJ356MO Polypropylene Copolymer BJ356MO is a heterophasic copolymer. This grade provides very high melt flow rate, very high stiffness and medium impact strength. and is designed for high-speed injection molding and contains nucle.. |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | mold average |
Borealis Daplen™ ED117AE Polypropylene TPO Compound Daplen™ ED117AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surfac.. |
|||
Linear Mold Shrinkage | 0.010 - 0.014 cm/cm @Thickness 3.20 mm, Time 259000 sec |
0.010 - 0.014 in/in @Thickness 0.126 in, Time 72.0 hour |
ISO 294 |
A. Schulman FORMION™ FI 391E Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.010 - 0.014 cm/cm | 0.010 - 0.014 in/in | ISO 294-4 |
Wellman Wellamid® 42LH-N Unfilled Nylon 6, Lubricated & Heat Stabilized Typical Applications: Automotive seat belt, buckle and anchor components; convoluted tubing for wire harnesses; furniture hardware, curtain glides.Data provided by the manufacturer, Wellman Inc. |
|||
Linear Mold Shrinkage | 0.010 - 0.014 cm/cm | 0.010 - 0.014 in/in | ISO 294-4 |
Wellman Wellamid® GS40-60 42L-N 40% Glass Sphere Filled Nylon 6, Lubricated Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | MD; ASTM D955 |
Aclo Accutech Polypropylene Copolymer CP0437C30L Calcium Reinforced |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | ASTM Data; MD |
BASF Ultramid® A27 E 01 PA66 (Conditioned) Ultramid A27 E 01 is a low-viscosity, general-purpose PA66 grade for compounding. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation ".. |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | across flow; ISO 294-4 |
Solvay Specialty Polymers Amodel® A-6135 NL Polyphthalamide (PPA), 35% Glass Fiber Reinforcement
(discontin Amodel A-6135 NL polyphthalamide (PPA), a 35% glass reinforced, high-glow, non-lubricated, hot-water moldable resin specially designed for laser welding. The black version is a laser absorber, and t.. |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
Ineos H28U-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Radiation stableTypical applications: MedicalComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from inject.. |