Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | ASTM D955 |
Multibase Multi-Pro® 4615 X White Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Linear Mold Shrinkage | 0.0080 - 0.011 cm/cm @Thickness 3.17 mm |
0.0080 - 0.011 in/in @Thickness 0.125 in |
|
Ovation Polymers Opnyl OP66UT105 Nylon 66 Ultra Tough - High Impact, Excellent retention of mechanical properties, High service temperature. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All.. |
|||
Linear Mold Shrinkage | 0.0080 cm/cm | 0.0080 in/in | as molded; ISO 294 |
Solvay Engineered Polymers SEQUEL® 1493 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1493 engineered polyolefin material is designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and excellent p.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPH K20040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0080 cm/cm | 0.0080 in/in | Across Flow; ISO 2577 |
Polykemi AB SCANMID 6 B12^ Q40 Nylon 6, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0080 - 0.014 cm/cm | 0.0080 - 0.014 in/in | |
Lehmann & Voss LUVOCOM® 65-8452-1 PP-copolymer, with aramid reinforcement, lubricant modified Applications: Office communication.Low warpage, isotropic shrinkage characteristics.Dynamic stressed parts.Information provided by Lehmann & Voss & Co.KG |
|||
Linear Mold Shrinkage | 0.0080 - 0.016 cm/cm | 0.0080 - 0.016 in/in | ASTM D955 |
Samyang Tramid® 210P Polyamide, High Productivity Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210P is a high productivity grade.Applications:ConnectorsCable tiesHarness clipsT.. |
|||
Linear Mold Shrinkage | 0.0080 cm/cm | 0.0080 in/in | mold average;Borealis Method |
Borealis Daplen™ EF005AE Polypropylene TPO Compound Daplen™ EF005AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give.. |
|||
Linear Mold Shrinkage | 0.0080 cm/cm @Thickness 3.175 mm |
0.0080 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm @Thickness 3.175 mm |
0.0080 - 0.012 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman SCHULAMID® 6 NV12 Easy Flow Low Viscosity Nylon 6 Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0080 cm/cm | 0.0080 in/in | |
Polyram RamLloy PBB702 PC/ABS alloy, UV Stabilized UV stabilized PC/ABS alloy for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0080 - 0.015 cm/cm | 0.0080 - 0.015 in/in | ASTM D955 |
Cheng Yu Plastic N6CV3 Flame Retardant Nylon 6, 30% Mineral Reinforced |
|||
Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
ELASTO UK Dryflex® 420401S SBS Based Material, 40D Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
ELASTO UK Dryflex® 500500S SEBS Based Material, Unfilled Qualities, 50A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
ELASTO UK Dryflex® 602650S SEBS Based Material, Filled Qualities, 65A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Linear Mold Shrinkage | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | |
ELASTO UK Dryflex® 662350S SEBS Based Material, Semi-Filled Qualities, 35A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm @Thickness 4.00 mm |
0.0080 - 0.010 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6000 GS 50 HWCP 50% Glass Sphere Filled Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm @Thickness 4.00 mm |
0.0080 - 0.012 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6600/508 HWUVCP Nylon 66, Impact Modified, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage | 0.0080 cm/cm | 0.0080 in/in | |
E-Polymers SEPAZ® N2020F Nanoclay 2% Fast cycle time Nano Composite Resin Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi.. |
|||
Linear Mold Shrinkage | 0.0080 cm/cm | 0.0080 in/in | Transfer; ASTM D955 |
Chang Chun Plastic Longlite PM T310 Impact Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Linear Mold Shrinkage | 0.0080 - 0.025 cm/cm | 0.0080 - 0.025 in/in | ASTM D955 |
Cheng Yu Plastic 3235 TPE Rubber |
|||
Linear Mold Shrinkage | 0.0080 cm/cm | 0.0080 in/in | ASTM D955 |
Adell EA-16 Homopolymer Polypropylene, 30% Talc Filled Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0080 cm/cm | 0.0080 in/in | ASTM D955 |
Ashley Polymers Ashlene® 114WO PBT Polyester A high impact polyester with low shrinkage, flame retardant.Data provided by the manufacturer |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PP HJ752 UV2 Polypropylene/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPH T5040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0080 cm/cm | 0.0080 in/in | Borealis Method |
Borealis Daplen™ PB4432 TPO Compound Daplen PE4432 is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen PE4432 is a material with excellent impact /stiffness ratio. Thanks to its low th.. |
|||
Linear Mold Shrinkage | 0.0080 cm/cm | 0.0080 in/in | LATI |
LATI LARAMID CE/60 60% Mineral Filled Polyphthalamide (PPA) Based Compound
(Unverified Data**) Laramid compounds are based on a unique semi-crystalline engineering polymer (polyphthalamide) offering improved performance compared to traditional engineering thermoplastics at a lower cost than s.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPH T5040 FC VT Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |