Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.50 µm | 0.50 µm | 52% of particles less than |
Old Hickory 44-B Kentucky Ball Clay The 44-B clay is similar to 54-S and is a recommended selection where additional plasticity and strength are important. It is particularly recommended in extruded and plastic processed ceramic formu.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 48% of particles less than |
Old Hickory 54-S Kentucky Ball Clay This ball clay is a multi- purpose clay that has excellent pressing, extrusion, and casting qualities. It has a moderately fine particle size distribution and the high plasticity and dry strength is.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 48% of particles less than |
Old Hickory 56-SR Kentucky Ball Clay This is a kaolinitic clay with excellent extrusion and die pressing characteristics. It has some colloidal carbon content but only a moderate amount of shrinkage. This clay is suitable for a variety.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 57% of particles less than |
Old Hickory APG-300 Kentucky Ball Clay This is an extremely low 325 Mesh wet residue clay. It can be employed in a variety of applications where high purity mineral filler is required. It has a moderate GE brightness value and is particu.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 24.4% of particles less than |
Old Hickory M&M Clays, Inc. Wilco-SLU Kaolin Clay Wilco SLU is an aqueous suspension of kaolin produced at 70% solids content. The slurry is deflocculated and rheology stabilized with sodium silicate. The Wilco SLU grade is a highly permeable selec.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 58% of particles less than |
Old Hickory M-23 Tennessee Ball Clay This is a very high quality porcelain grade ball clay. It has fine particle size distribution for excellent plasticity and strength in pressing or plastic forming application. the low Fe2O3 and TiO2.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 52% of particles less than |
Old Hickory No. 1 Glaze Kentucky Ball Clay No. 1 Glaze Clay is a very high kaolin bearing selection with extremely low levels of carbon content. it provides excellent suspension to all types of glazes especially glazes containing a high perc.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 48% of particles less than |
Old Hickory No. 5 Kentucky Ball Clay No. 5 clay is a kaolinitic ball clay containing low levels of carbon. It provides high suspension and plasticity to a variety of ceramic formulations and is an excellent source of Al2O3 content. No... |
|||
Particle Size | 0.50 µm | 0.50 µm | 56% of particles less than |
Old Hickory Thomas Tennessee Ball Clay Thomas clay is similar to Volunteer clay and has established an excellent history of performance in stoneware and low fire (talc base) plastic and casting formulas. The diverse combination of clays .. |
|||
Particle Size | 0.50 - 1.5 µm | 0.50 - 1.5 µm | D<sub>50</sub> |
NYC YT3CP Y2O3 Powder |
|||
Particle Size | 0.50 µm | 0.50 µm | 31% of particles less than |
Old Hickory UltraCast Slurry PC-2034 Kentucky Ball Clay These popular slurry grades are shipped at 60% solids content and deflocculated with sodium silicate to maintain stable rheology characteristics. All the above grades are suitable for a variety of c.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 28% finer than |
Imerys Allenâ„¢ G Kaolin Allen G is an intermediate-grained kaolin used as a suspension aid in ceramic glazes.Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 72% finer than |
Imerys Bardenâ„¢ R Kaolin Barden is a high surface area kaolin product used a filler in rubber and plastic applications.Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 71.5% finer than |
Imerys Barnetâ„¢ Kaolin Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 45% finer than |
Imerys Carverâ„¢ Kaolin Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 27% finer than |
Imerys DB-Floatâ„¢ Kaolin Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 38% finer than |
Imerys Diamondâ„¢ Kaolin Diamond is an intermediate-grained montmorillonitc kaolin used primarily in plastic formed bodies. This kaolin is known for its good strength and white-firing characteristics.Information provided by.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 25% finer than |
Imerys Ewingâ„¢ Kaolin Ewing is an intermediate grained air-floated kaolin which is selected, processed and controlled to meet specific requirements of the fibreglass industry.Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 69% finer than |
Imerys Hamiltonâ„¢ Kaolin Hamilton is a fine-grained kaolin with low alkali content and high PCE. These properties make for ideal air-set refractory mortars. Halloysite content provides excellent suspension and trowel abilit.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 23% finer than |
Imerys Kaolin Slurryâ„¢ Kaolin Slurry is a carefully controlled Kaolin-water suspension formulated for use in cermic castings.Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 30% finer than |
Imerys KT-Cast/Rogersâ„¢ Kaolin Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 72% finer than |
Imerys Mercapâ„¢ 100 Kaolin Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 10% |
Minelco UltraCarb LH3 Hydrated Magnesium Calcium Carbonate Mineral Flame RetardantUltracarb combines properties normally associated with several different materials that can be used jointly or individually to benefit many applications including rubber, plas.. |
|||
Particle Size | 0.50 µm | 0.50 µm | Mean |
Momentive Performance Materials AC6111 Boron Nitride (BN) Powder Agglomeration of submicron hexagonal turbostatic crystals. Used in paints, refractory coatings, mold/die release agents, nucleation aid, and lubricants. It is relatively non-wetting versus molten .. |
|||
Particle Size | 0.50 µm | 0.50 µm | |
Shin-Etsu Silicones X-52-2328 Fluid Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Particle Size | 0.50 - 1.0 µm | 0.50 - 1.0 µm | D50 Sedigraph |
Solvay Polishing Opaline™ Description: Polishing OPALINE® is a high quality cerium oxide powder developed high precision polishing. It has an excellent surface quality, very low roughness, and has quality consistency. The.. |
|||
Particle Size | 0.50 - 25 µm | 0.50 - 25 µm | PSD (d<sub>50</sub> |
Terio Corporation TZY-4 Yttria Stabilized Zirconia Information provided by TERIO Corporation. |
|||
Particle Size | 0.50 - 25 µm | 0.50 - 25 µm | PSD (d<sub>50</sub> |
Terio Corporation TCZA-20~80 CeO2-Al2O3-ZrO2 Information provided by TERIO Corporation. |
|||
Particle Size | <= 0.50 µm | <= 0.50 µm | Crystal size |
3M Nextel™ 550 Industrial Ceramic Fiber Chemical composition above is wt%. Crystal phases are gamma alumina amorphous SiO2. Filament diameter is 10-12 µm.3M Nextel fibers 312, 440, and 550 are designed for non-structural applications w.. |
|||
Particle Size | 0.50 µm | 0.50 µm | |
Astro Met AmZirOx 86 Zirconia - Zirconium Oxide General Description:AmZirOx 86 zirconia (Astro Met Zirconium Oxide) is a yttria stabilized zirconia ceramic material which features high strength and toughness making it a candidate material for use.. |