| Category | Ceramic , Clay , Kaolin Clay |
| Manufacturer | Imerys (Kentucky-Tennessee Clay Co.) |
| Trade Name | Kaolin Slurry™ |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Imerys Kaolin Slurryâ„¢.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Particle Size | 0.50 µm | 0.50 µm | 23% finer than |
| 1.0 µm | 1.0 µm | 43% finer than | |
| 2.0 µm | 2.0 µm | 57% finer than | |
| 5.0 µm | 5.0 µm | 78% finer than | |
| 10 µm | 10 µm | 89% finer than | |
| 20 µm | 20 µm | 96% finer than | |
| Particle Mesh Size | 325 Mesh | 325 Mesh | 5.0% retained |
| pH | 5.5 | 5.5 | |
| Specific Surface Area | 13 m²/g | 13 m²/g |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Modulus of Rupture | 0.00207 GPa | 0.300 ksi | dry |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Al2O3 | 38.2 % | 38.2 % | |
| CaO | 0.10 % | 0.10 % | |
| Fe2O3 | 0.50 % | 0.50 % | |
| K2O | 0.20 % | 0.20 % | |
| Loss on Ignition(%) | 13.5 % | 13.5 % | |
| MgO | 0.10 % | 0.10 % | |
| Na2O | 0.10 % | 0.10 % | |
| SiO2 | 45.3 % | 45.3 % | |
| TiO2 | 1.6 % | 1.6 % |
| Descriptive Properties | Value | Comments |
|---|---|---|
| M.B.I. (meq/100g) | 3.5 |