| Category | Ceramic , Clay , Kaolin Clay , Oxide , Aluminum Oxide , Silicon Oxide |
| Manufacturer | Imerys (Kentucky-Tennessee Clay Co.) |
| Trade Name | Barnet™ |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Imerys Barnetâ„¢ Kaolin.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
| Particle Size | 0.30 µm | 0.30 µm | median |
| 0.50 µm | 0.50 µm | 71.5% finer than | |
| 1.0 µm | 1.0 µm | 86% finer than | |
| 2.0 µm | 2.0 µm | 92% finer than | |
| 5.0 µm | 5.0 µm | 98% finer than | |
| 10 µm | 10 µm | 98.5% finer than | |
| 20 µm | 20 µm | 99.5% finer than | |
| Particle Mesh Size | 325 Mesh | 325 Mesh | 2% retained |
| pH | >= 4.0 | >= 4.0 |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Al2O3 | 38.5 % | 38.5 % | |
| CaO | 0.10 % | 0.10 % | |
| Fe2O3 | 1.2 % | 1.2 % | |
| K2O | 0.20 % | 0.20 % | |
| Loss on Ignition(%) | 13.6 % | 13.6 % | |
| MgO | 0.050 % | 0.050 % | |
| Na2O | 0.10 % | 0.10 % | |
| SiO2 | 44.8 % | 44.8 % | |
| TiO2 | 1.45 % | 1.45 % |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Moisture Content | 1.0 - 3.0 % | 1.0 - 3.0 % |