Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | |
Nabaltec NABALOX® NO 115 TC Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | |
Nabaltec NABALOX® NO 115-25 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | |
Nabaltec NABALOX® NO 315 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | |
Nabaltec NABALOX® NO 325 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | |
Nabaltec NABALOX® NO 615-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | |
Nabaltec NABALOX® NO 625-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.800 - 0.900 g/cc | 0.0289 - 0.0325 lb/in³ | PEPL-10-W-67 |
Pearl Engineering PEPLPET B-07C PET Bottle Grade A co-polymer used mostly for containers. |
|||
Bulk Density | 0.800 - 0.900 g/cc | 0.0289 - 0.0325 lb/in³ | PEPL-10-W-67 |
Pearl Engineering PEPLPET B-101C PET Sheet Grade A sheet grade polymer used in thick films. |
|||
Bulk Density | 0.800 - 0.900 g/cc | 0.0289 - 0.0325 lb/in³ | PEPL-10-W-67 |
Pearl Engineering PEPLPET B-103C PET Bottle Grade A co-polymer used for mineral water bottles |
|||
Bulk Density | 0.800 - 0.900 g/cc | 0.0289 - 0.0325 lb/in³ | |
Taiwan PU Corporation MOCA Polyurethane Resin Curing Agent MOCA [4,4' - Methylene bis-(ortho-chloroaniline)] is used as a PU curing agent. The chlorine atoms on benzene ring can slow down the activity of the NH2 group, so as to extend the pot life while ca.. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
Solvay Chemicals NOCOLOK® Flux Drystatic Potassium Fluoroaluminate Flux using electrostatic/dry powder coating. Classifications: HS No.: 38109090 /CAS-No.: 60304-36-1Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & .. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
Solvay Chemicals NOCOLOK® Li Flux Drystatic Flux for aluminum brazing with further reduced residue solubility and improved corrosion characteristics and using electrostatic/dry powder coating.HS No.: 38109090 /CAS-No.: 60304-36-1 and 13821-.. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | tapped |
Solvay Chemicals Strontium carbonate fine powder Strontium carbonate fine powder is used in the production of ferrites for permanent magnets, and in Zinc electrolysis for removal of lead. Strontium carbonate fine powder is also used in the product.. |
|||
Bulk Density | 0.820 - 0.900 g/cc | 0.0296 - 0.0325 lb/in³ | |
SK Chemicals SKYPET® BB7755 Specially Formulated PET Resin Description: SKYPET-BB7755 is a specially formulated PET resin for PET bottles especially for hot-fill application. SKYPET-BB7755 provides excellent processability in injection molding and blow mol.. |
|||
Bulk Density | 0.820 - 0.900 g/cc | 0.0296 - 0.0325 lb/in³ | |
SK Chemicals SKYPET® BL8050 Specially Formulated PET Copolymer Resin SKYPET-BL8050 is a specially formulated PET copolymer resin for PET bottles and extruded sheet. SKYPET-BL8050 provides excellent processability in injection molding and blow molding processes, offe.. |
|||
Bulk Density | 0.820 - 0.900 g/cc | 0.0296 - 0.0325 lb/in³ | |
SK Chemicals SKYPET® BR8040 Low Content CHDM Modified Copolyester Resin Description: SKYPET-BR8040 is a low content CHDM modified copolyester resin for large sized-mineral water bottles and extruded sheet. SKYPET-BR8040 has sufficiently low crystallization rate for lar.. |
|||
Bulk Density | 0.820 - 0.900 g/cc | 0.0296 - 0.0325 lb/in³ | |
SK Chemicals SKYPET® XT8050 Specially Formulated PET Copolymer Resin Description: SKYPET-XT8050 is a fast reheat grade of SKYPET, specially formulated for high productivity in the blowing process. SKYPET-XT8050 provides excellent processability in injection molding .. |
|||
Bulk Density | 0.820 - 0.900 g/cc | 0.0296 - 0.0325 lb/in³ | |
SK Chemicals SKYPET® BL8450 Specially Formulated PET Copolymer Resin Description: SKYPET-BL8450 is a specially formulated PET copolymer resin for PET bottles and extruded sheet. SKYPET-BL8450 provides excellent processability in injection molding and blow molding pr.. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4300 M5 25% Mineral Filled PBT Description: Is a PBT-HI, injection-molding grade reinforced with 25% of minerals, for the production of parts with good surface quality and low warpage, e.g. housings and visible parts of domestic .. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4520 High Speed PBT Description: Very easy flowing unreinforced injection molding grade with enhanced elongation for thin-walled parts (e.g. automotive connectors, switches, relay parts)Information provided by BASF |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® S 4090 G6X High Speed 30% Glass Filled PBT Description: Low-warpage, easy-flowing injection molding grade with 30 % glass fibers for technical parts, for which dimensional stability is very important, reduction of wall thickness (eg, e/e hou.. |
|||
Bulk Density | 0.800 - 0.900 g/cc | 0.0289 - 0.0325 lb/in³ | |
Addcomp ADD-VANCE® BA 401 Blowing agent Fields of application: Foamed products of Polyolefin and other polymers.Examples: Extruded sheets and foams in general as well as injection molded parts that require a foamed core.Mode of action and.. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4040 G10 50% Glass Filled BK 15029 PBT + PET Description: Injection molding grade with 50% glass fibers for industrial parts with excellent surface quality, for example external door handles in vehicles, visible sunroof frames, oven door handl.. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4500 BK 00110 PBT Information provided by BASF |
|||
Bulk Density | 0.750 - 0.900 g/cc | 0.0271 - 0.0325 lb/in³ | Powder Density; ISO 60 |
Vyncolit 3520 CG Novolac Phenolic Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par.. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4040 G6 30% Glass Filled PBT + PET PBT + PET, injection-molding grade containing 30% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housin.. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4300 G2 FC 10% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4300 G3 High Speed 15% Glass Filled BK 15045 PBT Description: Easy flowing injection molding grade with 15 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg timer dials, toggles, knobs, parts for thermostats, oven-door .. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4300 G6 HR 30% Glass Filled BK 15116 PBT Description: injection-molding grade with 30% glass-fibers; for rigid and dimensionally stable technical parts with increased requirements on hydrolysis resistance. For example automotive connectors.. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4300 G6 LT 30% Glass Filled BK 150926 PBT Description: Easy flowing injection molding grade with 30 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg windshield wiper arms, printed circuit boards PCBs), housing, .. |