SK Chemicals SKYPET® BL8450 Specially Formulated PET Copolymer Resin

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer SK Chemicals
Trade Name SKYPET®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SK Chemicals SKYPET® BL8450 Specially Formulated PET Copolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: SKYPET-BL8450 is a specially formulated PET copolymer resin for PET bottles and extruded sheet. SKYPET-BL8450 provides excellent processability in injection molding and blow molding processes, offers low Acetaldehyde contents (max 1 ppm) in the final container, has excellent thermal stability during melt processing, has slower crystallization rate suitable for highly transparent container.Applications: Carbonated soft drink bottles, mineral water bottles, custom bottles, extruded sheet and thermoformed articles. Information provided by SK Chemicals.
Physical Properties Metric English Comments
Bulk Density 0.820 - 0.900 g/cc
0.0296 - 0.0325 lb/in³
Density 1.40 g/cc
0.0506 lb/in³
Viscosity Test 82 - 86 cm³/g
82 - 86 cm³/g
intrinsic viscosity
Thermal Properties Metric English Comments
Melting Point 245 - 247 °C
473 - 477 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Moisture Content <= 0.30 %
<= 0.30 %