NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insulationhigh mechanical strengthhigh temperature propertiesdimensional accuracyoptimized chemical resistanceRefractory Industry, Engineering Ceramics
Physical Properties Metric English Comments
Bulk Density 0.700 - 0.900 g/cc
0.0253 - 0.0325 lb/in³
Density 2.35 g/cc
0.0849 lb/in³
Green Density
3.70 g/cc
0.134 lb/in³
Sintered Density
3.90 g/cc
0.141 lb/in³
Loss On Ignition <= 0.300 %

@Temperature 20.0 - 1100 °C
<= 0.300 %

@Temperature 68.0 - 2010 °F
Particle Size >= 2.0 µm
>= 2.0 µm
Primary Crystal Size
1.5 - 2.5 µm
1.5 - 2.5 µm
Specific Surface Area 1.2 - 1.8 m²/g
1.2 - 1.8 m²/g
BET
Thermal Properties Metric English Comments
Shrinkage 13 %
13 %
Sintering Shrinkage
Component Elements Properties Metric English Comments
Al2O3 >= 99.6 %
>= 99.6 %
Fe2O3 0.030 %
0.030 %
Na2O 0.30 %
0.30 %
SiO2 0.030 %
0.030 %
Processing Properties Metric English Comments
Sintering Temperature 1725 °C
3137 °F
Descriptive Properties Value Comments
alpha-Al2O3-Content % 98