Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0051 cm/cm @Time 86400 sec |
0.0051 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP DFL28 PC LNP* Lubricomp* DFL28 is a compound based on Polycarbonate resin containing 40% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.0051 cm/cm @Time 86400 sec |
0.0051 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP DFL28 PC (Asia Pacific) LNP* Lubricomp* DFL28 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.0051 cm/cm @Time 86400 sec |
0.0051 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP EX06405 PEI LNP* LUBRICOMP* EX06405 is a compound based on Polyetherimide resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible, Easy Molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0051 cm/cm @Time 86400 sec |
0.0051 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP EX06405 PEI (Asia Pacific) LNP* Lubricomp* EX06405 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Linear Mold Shrinkage, Transverse | 0.0051 cm/cm @Time 86400 sec |
0.0051 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP GFL36L PSU (Asia Pacific) LNP* Lubricomp* GFL36L is a compound based on Polysulfone resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Linear Mold Shrinkage, Transverse | 0.0051 cm/cm @Time 86400 sec |
0.0051 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DEP42E PC LNP STAT-KON* DEP42E is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 20% PTFE/Silicone. Added features of this material include: Easy Molding. Electrically Conductive, Wear.. |
|||
Linear Mold Shrinkage, Transverse | 0.0051 cm/cm @Time 86400 sec |
0.0051 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DEP42E PC (Asia Pacific) LNP STAT-KON* DEP42E is a compound based on Polycarbonate resin containing Silicone, PTFE, Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0051 cm/cm @Time 86400 sec |
0.0051 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DX05474 PC LNP* STAT-KON* DX05474 is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Retardant, Mold .. |
|||
Linear Mold Shrinkage, Transverse | 0.0051 cm/cm @Time 86400 sec |
0.0051 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DX05474 PC (Asia Pacific) LNP* Stat-kon* DX05474 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Ret.. |
|||
Linear Mold Shrinkage, Transverse | 0.0051 cm/cm @Time 86400 sec |
0.0051 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP DF002ERH PC LNP THERMOCOMP* DF002ERH is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Healthcare, Mold Release. |
|||
Linear Mold Shrinkage, Transverse | 0.0051 cm/cm @Time 86400 sec |
0.0051 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP DF002ERJ PC LNP THERMOCOMP* DF002ERJ is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Healthcare. |
|||
Linear Mold Shrinkage, Transverse | 0.0051 cm/cm @Time 86400 sec |
0.0051 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP DF006P PC LNP THERMOCOMP* DF006P is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Exceptional Processing. |
|||
Linear Mold Shrinkage, Transverse | 0.0051 cm/cm @Time 86400 sec |
0.0051 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP DX06408 PC LNP THERMOCOMP* DX06408 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Linear Mold Shrinkage, Transverse | 0.0051 cm/cm @Time 86400 sec |
0.0051 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP DX06409 PC LNP* THERMOCOMP* DX06409 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Healthcare. |
|||
Linear Mold Shrinkage, Transverse | 0.0051 cm/cm @Time 86400 sec |
0.0051 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP EC006E PEI LNP THERMOCOMP* EC006E is a compound based on Polyetherimide resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive |
|||
Linear Mold Shrinkage, Transverse | 0.0051 - 0.0058 cm/cm @Time 86400 sec |
0.0051 - 0.0058 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive |
|||
Linear Mold Shrinkage, Transverse | 0.0051 - 0.0058 cm/cm @Time 86400 sec |
0.0051 - 0.0058 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK (Asia Pacific) LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0051 cm/cm @Time 86400 sec |
0.0051 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP DF002ER PC LNP THERMOCOMP* DF002ER is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding. Mold Release |
|||
Linear Mold Shrinkage, Transverse | 0.0051 cm/cm @Time 86400 sec |
0.0051 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP GFL36L PSU LNP* Lubricomp* GFL36L is a compound based on Polysulfone resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Linear Mold Shrinkage, Transverse | 0.0051 cm/cm @Time 86400 sec |
0.0051 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP DX06409 PC (Asia Pacific) LNP* Thermocomp* DX06409 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |