Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Beijing Evergrow Resources MoS2 Filled Nylon

Category Polymer , Thermoplastic , Nylon
Manufacturer Beijing Evergrow Resources
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Evergrow Resources MoS2 Filled Nylon.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Beijing Evergrow Resources.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
GB1033
Mechanical Properties Metric English Comments
Hardness, Shore D 80 - 88
80 - 88
GB3398
Ball Indentation Hardness 148.5 MPa
21540 psi
GB3398
Tensile Strength at Break 74.1 MPa
10700 psi
GB/T 1040
Elongation at Yield <= 25 %
<= 25 %
GB/T 1040
Modulus of Elasticity 3.10 GPa
450 ksi
GB/T 1040
Flexural Strength 86.9 MPa
12600 psi
GB9341
Compressive Strength 90.0 - 105 MPa
13100 - 15200 psi
GB/T 1040
Izod Impact, Notched (ISO) 6.40 kJ/m²
3.05 ft-lb/in²
GBT1043
Coefficient of Friction 0.107
0.107
GB3360
Thermal Properties Metric English Comments
CTE, linear 75.0 µm/m-°C
41.7 µin/in-°F
GB1036
Melting Point 230 °C
446 °F
HG/T2235
Heat Distortion Temperature 145 °C
293 °F
GB1634
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Volume; GB1410
Arc Resistance 600 sec
600 sec
ASTM D112
Processing Properties Metric English Comments
Moisture Content 1.9 - 2.0 %
1.9 - 2.0 %
in air
6.1 - 6.3 %
6.1 - 6.3 %
in water
Users viewing this material also viewed the following: