Polymer Property : Density = 0.0383 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.937 - 1.06 g/cc
0.0339 - 0.0383 lb/in³
Average value: 0.957 g/cc Grade Count:19
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Sheet/Thermoforming Grade". Each property range of values reported is ..
Density 1.025 - 1.06 g/cc

@Temperature 15.0 - 15.0 °C
0.03703 - 0.0383 lb/in³

@Temperature 59.0 - 59.0 °F
Average value: 1.05 g/cc Grade Count:3
Overview of materials for Epoxy Cure Resin
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M..
Density 1.04 - 1.06 g/cc
0.0376 - 0.0383 lb/in³
Solvay ALKAMULS® EL 620 LI E Surfactant
Description: Biodegradable castor oil ethoxylate emulsifier, solubiliser for a wide range of formulations with an HLB of around 12.Identification: CASTOR OIL ETHOXYLATE (30)CAS: 61791 – 12 â€..
Density 1.04 - 1.06 g/cc
0.0376 - 0.0383 lb/in³
RP-0064
Solvay ALKAMULS® EL 620LI Surfactant
Description: Biodegradable castor oil ethoxylate emulsifier, solubiliser for a wide range of formulations with an HLB of around 12.Chemical Name: CASTOR OIL ETHOXYLATE(30)CAS: 61791-12-6, 7732-18-5A..
Density 1.04 - 1.06 g/cc
0.0376 - 0.0383 lb/in³
AN4037
Solvay STANNINE® 5525 Surfactant
Description: Blend of substituted thiourea and surfactantsIdentification: ACID PICKLING INHIBITOR (SUBSTITUTED THIOUREA)CAS: 61791 – 00 – 2Solubility: Complete in acidsAvailable in: Asia P..
Density 1.03 - 1.06 g/cc
0.0372 - 0.0383 lb/in³
Spec; ISO 1183-1
Axion Polymers Axpoly® PS01 3003 Enhanced White General Purpose Polystyrene
PS01 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS01 range of resin co..
Density 1.03 - 1.06 g/cc
0.0372 - 0.0383 lb/in³
Spec; ISO 1183-1
Axion Polymers Axpoly® PS01 3009 Green General Purpose Polystyrene
PS01 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS01 range of resin co..
Density 1.03 - 1.06 g/cc
0.0372 - 0.0383 lb/in³
Spec; ISO 1183-1
Axion Polymers Axpoly® PS01 Impact Modified Polystyrene
100% post-consumer recycled polymer (recovered from refrigerators)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in a range of co..
Density 1.02 - 1.06 g/cc
0.0368 - 0.0383 lb/in³
Spec; ISO 1183-1
Axion Polymers Axpoly® PS02 1000 General Purpose Polystyrene
PS02 Series polystyrenes offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS02 range of resin com..
Density 1.02 - 1.06 g/cc
0.0368 - 0.0383 lb/in³
Spec; ISO 1183-1
Axion Polymers Axpoly® PS02 1010 Medium Impact Polystyrene
PS02 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS02 range of resin co..
Density 1.02 - 1.06 g/cc
0.0368 - 0.0383 lb/in³
Spec; ISO 1183-1
Axion Polymers Axpoly® PS02 Impact Modified Polystyrene
100% post-consumer recycled polymer (recovered from television casings)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in black/gr..
Density 1.02 - 1.06 g/cc
0.0368 - 0.0383 lb/in³
Spec; ISO 1183-1
Axion Polymers Axpoly® PS13 1000 Impact Modified Polystyrene
PS13 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS13 range of resin co..
Density 1.02 - 1.06 g/cc
0.0368 - 0.0383 lb/in³
Spec; ISO 1183-1
Axion Polymers Axpoly® PS13 Impact Modified Polystyrene
100% post-consumer recycled polymer (recovered from coat hangers)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in black/greyCost..
Density 1.04 - 1.06 g/cc
0.0376 - 0.0383 lb/in³
Internal
AKG Polymers Vision PP PPH BL1302 T20 Polypropylene Compound
Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin..
Density 1.02 - 1.06 g/cc
0.0368 - 0.0383 lb/in³
ISO 1183
Austin Novel Materials Texalan® 770A PCL TPU
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
Density 1.03 - 1.06 g/cc
0.0372 - 0.0383 lb/in³
Spec; ISO 1183-1
Axion Polymers Axpoly® PS01 3000 General Purpose Polystyrene
PS01 Series polystyrenes offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS01 range of custom co..
Density 1.02 - 1.06 g/cc
0.0368 - 0.0383 lb/in³
Spec; ISO 1183-1
Axion Polymers Axpoly® PS13 1011 High Impact Polystyrene
PS13 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS13 range of resin co..
Copyright © lookpolymers.com All Rights Reserved