Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.77 - 1.79 g/cc | 0.0639 - 0.0647 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Density | 1.77 - 1.79 g/cc | 0.0639 - 0.0647 lb/in³ | ASTM D792 |
Kureha KF Polymer 1100 PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Density | 1.77 - 1.79 g/cc | 0.0639 - 0.0647 lb/in³ | ASTM D792 |
Kureha KF Polymer 1550 High Viscosity PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Density | 1.77 - 1.79 g/cc | 0.0639 - 0.0647 lb/in³ | ASTM D792 |
Kureha KF Polymer 1700 High Viscosity PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Density | 1.77 - 1.79 g/cc | 0.0639 - 0.0647 lb/in³ | ASTM D792 |
Kureha KF Polymer 850 PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Density | 1.77 - 1.79 g/cc | 0.0639 - 0.0647 lb/in³ | ASTM D792 |
Kureha KF Polymer 1000 PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Density | 1.77 - 1.79 g/cc | 0.0639 - 0.0647 lb/in³ | ASTM D792 |
Kureha KF Polymer 1300 PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Density | 1.77 - 1.79 g/cc | 0.0639 - 0.0647 lb/in³ | ASTM D792 |
Kureha KF Polymer 2950 PVDF Copolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Density | 1.77 - 1.79 g/cc | 0.0639 - 0.0647 lb/in³ | ASTM D792 |
CPC - Vycom FLAMETEC™ KYTEC® PVDF Kytec® PVDF, the homopolymer of 1, 1-difluoroethene, is a tough engineering thermoplastic that offers a unique balance of properties. Kytec has the characteristic stability of fluoropolymers when e.. |
|||
Density | 1.75 - 1.79 g/cc | 0.0632 - 0.0647 lb/in³ | ISO R 1183 |
Fainplast Compounds CR 85 Flexible PVC, Electrical Bedding Bedding |
|||
Density | 1.59 - 1.79 g/cc | 0.0574 - 0.0647 lb/in³ | Molded |
Bulk Molding Compounds BMC T44 High Strength Mineral Filled Molding Compound BMC T44 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displacing .. |
|||
Density | 1.59 - 1.79 g/cc | 0.0574 - 0.0647 lb/in³ | Molded |
Bulk Molding Compounds BMC T44-15613 High Strength Mineral Filled Molding Compound BMC T44-15613 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displ.. |
|||
Density | 1.77 - 1.79 g/cc | 0.0639 - 0.0647 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Hylar® MP20 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Density | 1.41 - 1.79 g/cc | 0.0509 - 0.0647 lb/in³ | Average value: 1.61 g/cc Grade Count:10 |
Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Stainless Steel Fiber". Each property range of values reported is minimum a.. |
|||
Density | 1.48 - 1.79 g/cc | 0.0535 - 0.0647 lb/in³ | Average value: 1.64 g/cc Grade Count:22 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |