Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.91 g/cc | 0.322 lb/in³ | |
Materion moldMAX® XL Spinodally Hardened Copper-Nickel-Tin Alloy moldMAX XL® is a unique spinodally hardened copper-nickel-tin alloy that combines high strength and high thermal conductivity. Available in large plate thickness up to 12†and in rounds up t.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
Materion ToughMet® T2 CX 90 ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
HP Alloys Alloy C-276, 50% Cold Worked 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
Special Metals MONEL® 404 Copper-Nickel Alloy Data provided by California Fine Wire and the manufacturer, Special Metals. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | Annealed |
Eagle Brass 110 EPT COPPER, 3/4 Hard Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | Annealed |
Eagle Brass 110 EPT COPPER, Hard Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | Annealed |
Eagle Brass 194 HSM® Copper, Spring High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
CLAL-MSX NICLAFOR® 1000 TB Quenched Drawn Copper Alloy Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
CLAL-MSX NICLAFOR® 1000 TD1 Quenched/Cold Rolled, Drawn Copper Alloy Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
CLAL-MSX NICLAFOR® 1000 TD2 Quenched/Cold Rolled, Drawn Copper Alloy Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
CLAL-MSX NICLAFOR® 1000 TF Quenched/Precipitation Heat Treated, Rolled Copper Alloy Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
CLAL-MSX NICLAFOR® 1000 TH1 Quenched/Precipitation Heat Treated, Rolled Copper Alloy Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
CLAL-MSX NICLAFOR® 1000 TH4 Quenched/Cold Rolled/Precipitation Heat Treated, Rolled Copper Alloy Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
CLAL-MSX NICLAL 3444 H14 4/4 Hard Copper Alloy, diameter < 8 Copper Alloy, Free Cutting Bronze Main Characteristics: Excellent machineabilityHigh mechanical propertiesSelf lubricating alloyTypical Applications:Parts for connectorsFriction partsBearings-Pinions-Lock pinsInformation provided b.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
CLAL-MSX SICLANIC S® TF Quenched Copper Alloy, precipitation treated SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
CLAL-MSX ARCAP Anticorrosion AP4 H12 1/2 hard, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
Cadi C11000 ETP Standard Grade Copper The standard grade of copper - most widely used electrical conductor - suitable where mechanical design is not an issue and maximization of electrical or thermal conductivity is the primary concern... |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
California Fine Wire Nickel A 200 Nickel Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
Ametek High Purity Nickel Strip 899A 3/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
Ametek High Purity Nickel Strip 899A Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
Ametek High Purity Nickel Strip 899L 1/2 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
Ametek High Purity Nickel Strip 899L Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
Ametek High Purity Nickel Strip 899L Full Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
Ametek High Purity Nickel Strip 899M 1/2 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
Ametek High Purity Nickel Strip 899M Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
ATI Allegheny Ludlum AL 200™ Nickel Alloy, UNS N02200 Ferromagnetic. Allegheny Ludlum AL 200 alloy is wrought commercially pure nickel. This alloy provides highly ductile mechanical properties across a wide temperature range. Either alloy provides c.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
ATI Allegheny Ludlum AL 276™ Nickel-Base Alloy, UNS N10276 AL 276 alloy is a nickel-chromium-iron-tungsten alloy which is among the most corrosion resistant of alloys currently available. The AL 276 alloy is widely used in the severest environments encount.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
Ametek High Purity Nickel Strip 899A Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
ATI Allegheny Ludlum AL 201™ Nickel Alloy, UNS N02201 Ferromagnetic. Allegheny Ludlum AL 201 alloy is wrought commercially pure nickel. This alloy provides highly ductile mechanical properties across a wide temperature range. Either alloy provides c.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
HP Alloys Alloy C-276, 30% Cold Worked 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |