Materion ToughMet® T2 CX 90

Category Metal , Nonferrous Metal , Copper Alloy
Manufacturer Materion Corporation (former Brush Wellman)
Trade Name ToughMet®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Materion ToughMet® T2 CX 90.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engineered ToughMet® to provide attributes beyond those typically found in a high-strength copper alloy.Exceptional resistance to corrosion and cavitationOutstanding lubricity and durability in demanding applicationsHighly uniform composition in all product formsUniform microstructure in a variety of wrought shapes and sizesToughMet® 3 in the wrought and spinodally hardened (AT) condition exhibits tensile strength up to 140 ksi and hardness up to HRc 34 in a Copper-15% Nickel-8% Tin alloy with excellent machinability.Information supplied by Brush Wellman Engineered Materials.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.
Physical Properties Metric English Comments
Density 8.91 g/cc
0.322 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C >= 27
>= 27
Tensile Strength, Ultimate >= 724 MPa
>= 105000 psi
Tensile Strength, Yield >= 621 MPa
>= 90000 psi
Elongation at Break >= 3 %
>= 3 %
Modulus of Elasticity 117 GPa
17000 ksi
Poissons Ratio 0.30
0.30
Fatigue Strength 138 MPa

@# of Cycles 1.00e+6
20000 psi

@# of Cycles 1.00e+6
R = -1, 105 ksi YS
Shear Modulus 45.1 GPa
6540 ksi
calculated
Charpy Impact 13.6 - 27.1 J
10.0 - 20.0 ft-lb
V-Notch
Thermal Properties Metric English Comments
CTE, linear 16.2 µm/m-°C

@Temperature 21.1 - 102 °C
9.00 µin/in-°F

@Temperature 70.0 - 215 °F
Thermal Conductivity 51.9 W/m-K
360 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 85 %
85 %
As remainder
Nickel, Ni 9.0 %
9.0 %
Tin, Sn 6.0 %
6.0 %
Electrical Properties Metric English Comments
Magnetic Permeability <= 1.001
<= 1.001