Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.87 g/cc | 0.0676 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE D 4210 BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE D 5010 Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | |
Polygon Polylube™ Fiber Series Epoxy Composite Bearings Low friction coupled with high load carrying capacity are natural benefits. Teflon® superfilaments, which exhibit tensile strength twenty times greater than PTFE resins are integrated into the bea.. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | |
Meilian Chemical PE12077 WHITE MASTERBATCH WHITE PE12077 is a LDPE based masterbatch containing high-quality TiO2 without any addition of filler or fluorescence whitener. It is designed for use in economy films for general purpose, especiall.. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | ASTM D572 |
Haysite ETS Glass Reinforced Polyester Sheet, Electrical Grade (GPO1) A NEMA GPO-1 economy grade fiberglass mat reinforced thermoset polyester molded sheet. ETS is an IEEE Class B 130ºC electrical/160ºC mechanical material with good punching characteristics. Typ.. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | ASTM D572 |
Haysite HCR-100 Corrosion Resistant Polyester/Glass Sheet A general purpose isophthalic polyester sheet with flame retardants and ultraviolet inhibitors. Standard color is gray. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | |
LATI Larton CE/60 PPS, 60% Mineral Reinforced Polyphenylene Sulfide (PPS) based compound. Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; .. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | ASTM D891 |
Solvay Specialty Polymers FOMBLIN® LC55 PFPE Lubricant FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requir.. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | ASTM D891 |
Solvay Specialty Polymers FOMBLIN® M100 PFPE Lubricant Fomblin® PFPE fluorinated lubricants are used when harsh chemical environments, high temperatures or wide working-temperature ranges are encountered.Information provided by Solvay Solexis, Inc. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | ASTM D792 |
Techmer ES HiFill® ECTFE GF25 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightFeatures: CopolymerAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP UFW49RS PPA (Europe-Africa-Middle East) LNP* Thermocomp* UFW49RS is a compound based on Polyphthalamide resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP UFW49RSC PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UFW49RSC is a compound based on Polyphthalamide resin containing Glass Fiber, Mineral. Added features include: Heat Stabilized. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | Relative Density; ASTM D792 |
Sumitomo Bakelite North America RX® 1366FR-P Short-Glass Reinforced Diallyl Phthalate Short glass fiber reinforced, flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type SDG-F.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America RX® 3-1-525F-P Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG-F.I.. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP 2F005 ETFE LNP* Thermocomp* 2F005 is a fluoropolymer compound based on ETFE containing 25% Glass Fiber. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | ASTM D792 |
Plenco 1500 Polyester, Granular, Transfer Molded PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon.. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | ASTM D792 |
Plenco 1501 Polyester, Pellet, Injection Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | |
Trelleborg Emerson & Cuming Eccobond® TP 50 Two-Component Low Temperature Performance Silicone Adhesive Emerson & Cuming TP 50 Eccobond® Two-Component Low Temperature Performance Silicone AdhesiveFilled, RTV silicone rubber, paste adhesive. Room temperature cure. Very flexible. Color coded for ease o.. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | |
Hexcel® UHM Carbon Fiber (12,000 Filaments) Weight/length = 0.341 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin.. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | |
Hexcel® UHM Carbon Fiber (3000 Filaments) Weight/length = 0.085 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin.. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | ISO 1183 |
DSM Stanyl® 46HF5041LW (DAM) Nylon 46 40% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow, Low Warpage (North America) Information provided by DSM Engineering Plastics. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | (DAM); ISO 1183 |
DSM Stanyl® 46HF5041LW Nylon 46-40% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | ISO 1183 |
DSM Stanyl® 46HF5041LW Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | ISO 1183 |
DSM Stanyl® 46HF5050 (DAM) Nylon 46 50% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow (North America) Information provided by DSM Engineering Plastics. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | (DAM); ISO 1183 |
DSM Stanyl® 46HF5050 Nylon 46-50% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | ASTM D792 |
Applied Composites 185 Polyester SMC Industry Application: TransportationProduct Application: Lawn and GardenDistinct Features: Limited PigmentabilityInformation provided by Applied Composites Corporation. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | ASTM D1475 |
Aptek 6505PMF Electronic-grade, non-conductive adhesive APTEK 6506-PMF is a one component, 100% solid, mineral-filled epoxy adhesive specifically designed for the attachment of electronic components to printed circuit boards as well as a protective barri.. |
|||
Density | 1.87 - 2.07 g/cc | 0.0676 - 0.0748 lb/in³ | Molded |
Bulk Molding Compounds BMC T10(14) General Purpose Molding Compound BMC T10(14) is a general purpose, low shrink molding compound. Due to the excellent flow and controlled reactivity, BMC T10(14) is well suited for injection, transfer or compression molding of intr.. |
|||
Density | 1.87 g/cc | 0.0676 lb/in³ | ISO 1183 |
DSM Stanyl® 46HF5050 Nylon 46-50% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Density | 1.87 - 2.07 g/cc | 0.0676 - 0.0748 lb/in³ | Molded |
Bulk Molding Compounds BMC T70 Automotive Grade Molding compound BMC T70 is a low profile automotive grade molding compound specifically formulated for the vacuum metallization process. These compounds have excellent physical properties as well as superior adhes.. |